MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Kanthal Nicrosil Thermocouple wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Nicrosil is an austenitic nickel chromium silicon alloy (NiCrSi alloy) used for the positive leg of thermocouples type N. It offers higher thermoelectric stability in air above 1000°C (1830°F) and a better oxidation resistance in air than type E, J and K thermocouples. Nicrosil alloy can not be exposed to reducing or alternatively oxidizing and reducing atmospheres or to vacuum. This thermocouple is the most recent one among the different types covered by the international standards.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.53 g/cc0.308 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 800 MPa
@Thickness 2.00 mm
116000 psi
@Thickness 0.0787 in
Tensile Strength, Yield 310 MPa
@Thickness 2.00 mm
45000 psi
@Thickness 0.0787 in
Elongation at Break 35 %
@Thickness 2.00 mm
35 %
@Thickness 0.0787 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000100 ohm-cm0.000100 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 13.0 W/m-K90.2 BTU-in/hr-ft²-°F
Melting Point 1420 °C2590 °F
Maximum Service Temperature, Air  800 °C
@Diameter 0.250 mm
1470 °F
@Diameter 0.00984 in
Bare wire
 890 °C
@Diameter 0.500 mm
1630 °F
@Diameter 0.0197 in
Bare wire
 910 °C
@Diameter 0.250 mm
1670 °F
@Diameter 0.00984 in
Protected wire
 960 °C
@Diameter 1.00 mm
1760 °F
@Diameter 0.0394 in
Bare wire
 1000 °C
@Diameter 0.500 mm
1830 °F
@Diameter 0.0197 in
Protected wire
 1010 °C
@Diameter 1.63 mm
1850 °F
@Diameter 0.0642 in
Bare wire
 1100 °C
@Diameter 3.26 mm
2010 °F
@Diameter 0.128 in
Bare wire
 1110 °C
@Diameter 1.00 mm
2030 °F
@Diameter 0.0394 in
Protected wire
 1180 °C
@Diameter 1.63 mm
2160 °F
@Diameter 0.0642 in
Protected wire
 1250 °C
@Diameter 3.26 mm
2280 °F
@Diameter 0.128 in
Protected wire
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 14.2 %14.2 %
Nickel, Ni 84.3 %84.3 %As Balance
Silicon, Si 1.5 %1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Kanthal Thermothal N Thermocouple wire
Copper, Cu; Annealed
Constantan Thermocouple Wire
Sandvik Kanthal Cuprothal CL Thermocouple wire
Hoskins Manufacturing Chromel® Thermocouple Wire

NSANDV5035 / 199599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.