MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Ateva® 1615 Ethylene Vinyl Acetate Copolymer Coating Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: Well suited for extrusion coating, coextrusion and specialty lamination applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D1505, ASTM D1928 Proc A
Vinyl Acetate Content 16 %16 %
Melt Flow 15 g/10 min15 g/10 minASTM D1238 190/2.16
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3333ASTM D2240
Tensile Strength, Ultimate 12.0 MPa1740 psiASTM D638 Type IV
Elongation at Break 720 %720 %ASTM D638 Type IV
 
Thermal PropertiesMetricEnglishComments
Melting Point 88.0 °C190 °FASTM D3417
Vicat Softening Point 62.0 °C144 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %ASTM D1003
Gloss 65 %65 %45° Gloss, ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 2020 EVA polymer for coating lamination
Celanese Ateva® 1641 Ethylene Vinyl Acetate Copolymer Coating Resin
Dow Elvax® 3124 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
Celanese Ateva® 1943MS EVA polymer for coating lamination and flexible packaging
Celanese Ateva® 2811 Ethylene Vinyl Acetate Copolymer Coating Resin

PATEVA19 / 25936

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.