MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

A. Schulman Diamond NPP30-0800 GF40 40% Glass Filled Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Homopolymer Polypropylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Filler Content 40 %40 %Glass; ASTM D2584
Linear Mold Shrinkage 0.0020 cm/cm
@Thickness 1.59 mm
0.0020 in/in
@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 81.0 MPa11700 psichs 0.2 in/min; ASTM D638
Elongation at Yield 5.0 %5.0 %chs 0.2 in/min; ASTM D638
Flexural Strength 102.7 MPa14900 psiASTM D790
Flexural Modulus 6.752 GPa979.3 ksitangent; ASTM D790
Izod Impact, Notched 0.854 J/cm
@Thickness 3.17 mm
1.60 ft-lb/in
@Thickness 0.125 in
ASTM D256
Gardner Impact 0.500 J
@Temperature 23.0 °C
0.369 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 162 °C324 °F0.125";; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® M90-07 POM, Color Concentrate
Celanese Celcon® M90™ POM, Unfilled
Aclo Accutech Polypropylene Homopolymer HP0334G30CL Glass Reinforced Coupled
A. Schulman Diamond NPP30-0400 MGF30 30% Mineral & Glass Filled Homopolymer Polypropylene
Celanese Celcon® M90-34 POM, Unfilled

PDIAM408 / 126499

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.