System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
MRC Polymers NAXALOY 770GF16 Polycarbonate/ABS blend
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Glass Fiber Filled
Material Notes:
NAXALOY 770GF16 is a 16% glass filled polycarbonate/ABS blend. This material is available in black, natural and custom colors. It’s typically used for automotive interior applications.
Information provided by MCR Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.24
g/cc
1.24
g/cc
ASTM D792
Filler Content
16 %
16 %
ASTM D785
Melt Flow
3.0
g/10 min
@Load 5.00 kg,
Temperature 250 °C
3.0
g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
97.0
MPa
14100
psi
ASTM D638
Flexural Strength
148
MPa
21500
psi
ASTM D790
Flexural Modulus
4.762
GPa
690.7
ksi
ASTM D790
Izod Impact, Notched
1.07
J/cm
2.00
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
129
°C
264
°F
unannealed; ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
MRC Polymers NAXALOY™ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
MRC Polymers NAXALOY™ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
MRC Polymers NAXALOY 770GF10 Polycarbonate/ABS blend
Ensinger TECAPEI® made from Ultem® 1000 PEI
PMRC5007 / 217593
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.