MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Indium Corp. Indalloy 242 Tin-Lead Solder Alloy
Categories: Metal; Nonferrous Metal; Lead Alloy; Solder/Braze Alloy

Material Notes:

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 10.75 g/cc0.3884 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1010
Tensile Strength at Break 30.3 MPa4400 psi
Elongation at Break 30 %30 %
Modulus of Elasticity 19.0 GPa2760 ksi
Shear Strength 16.5 MPa2400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000193 ohm-cm0.0000193 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 29.0 µm/m-°C
@Temperature 20.0 °C
16.1 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 25.0 W/m-K
@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 275 - 302 °C527 - 576 °F
Solidus 275 °C527 °F
Liquidus 302 °C576 °F
 
Component Elements PropertiesMetricEnglishComments
Lead, Pb 89.5 %89.5 %
Tin, Sn 10.5 %10.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Indalloy 11 Lead Solder Alloy
Materion WS145 Solder
Materion WS187 Solder
Indium Corp. Indalloy 229 Lead Solder Alloy
Materion WS149 Solder

NNIN849 / 98058

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.