MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Baypren® 611 M 43±6 Chloroprene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Poly (2-chlorobutadiene-1,3), sulfur-modified with slight to medium crystallization tendency

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Volatiles <= 0.50 %
@Temperature 105 °C,
Time 10800 sec
<= 0.50 %
@Temperature 221 °F,
Time 3.00 hour
ISO 248/ASTM D5668
Mooney Viscosity 37 - 49
@Temperature 100 °C
37 - 49
@Temperature 212 °F
[MU], ML (1+4); ISO 289/ASTM D 1646
Ash <= 1.0 %<= 1.0 %Meth C; ISO 247
 
Processing PropertiesMetricEnglishComments
Cure Time  0.800 - 2.80 min
@Temperature 150 °C,
Time 1800 sec
0.0133 - 0.0467 hour
@Temperature 302 °F,
Time 0.500 hour
t10; ISO 2475
 0.800 - 2.80 min
@Temperature 150 °C,
Time 1800 sec
0.0133 - 0.0467 hour
@Temperature 302 °F,
Time 0.500 hour
ts02; ISO 2475
 3.50 - 7.90 min
@Temperature 150 °C,
Time 1800 sec
0.0583 - 0.132 hour
@Temperature 302 °F,
Time 0.500 hour
t80; ISO 2475
 20.0 - 24.0 min
@Temperature 150 °C,
Time 1800 sec
0.333 - 0.400 hour
@Temperature 302 °F,
Time 0.500 hour
S'max; ISO 2475
Shelf Life 6.00 Month
@Temperature <=25.0 °C
6.00 Month
@Temperature <=77.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Baypren® 216 M 43±5 Chloroprene Rubber
Lanxess Baypren® 110 M 41±5 Chloroprene Rubber
Lanxess Baypren® 126 Chloroprene Rubber
Lanxess Baypren® GF M22S VP Chloroprene Rubber
Precision Polymer Engineering C40M Chloroprene Rubber

PLANY8434 / 208827

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.