MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Haynes Hastelloy® S alloy, flat products
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications include seal rings in gas turbine engines, and severe cyclical heating conditions where it retains strength, ductility, and integrity.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS N06635, AMS 5711, AMS 5838, AMS 5873
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A  52
@Thickness 1.45 mm
52
@Thickness 0.0571 in
 57
@Thickness 12.7 mm
57
@Thickness 0.500 in
Tensile Strength, Ultimate  110 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 1093 °C
16000 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1999 °F
 117 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 1093 °C
17000 psi
@Thickness 0.374 - 1.00 in,
Temperature 1999 °F
 193 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 982 °C
28000 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1800 °F
 228 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 982 °C
33100 psi
@Thickness 0.374 - 1.00 in,
Temperature 1800 °F
 341 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 871 °C
49500 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1600 °F
 363 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 871 °C
52600 psi
@Thickness 0.374 - 1.00 in,
Temperature 1600 °F
 547 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 760 °C
79300 psi
@Thickness 0.374 - 1.00 in,
Temperature 1400 °F
 574 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 760 °C
83300 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1400 °F
 683 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 649 °C
99100 psi
@Thickness 0.374 - 1.00 in,
Temperature 1200 °F
 720 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 649 °C
104000 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1200 °F
 727 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 538 °C
105000 psi
@Thickness 0.374 - 1.00 in,
Temperature 1000 °F
 751 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 427 °C
109000 psi
@Thickness 0.374 - 1.00 in,
Temperature 801 °F
 756 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 316 °C
110000 psi
@Thickness 0.374 - 1.00 in,
Temperature 601 °F
 773 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 538 °C
112000 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1000 °F
 789 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 204 °C
114000 psi
@Thickness 0.374 - 1.00 in,
Temperature 399 °F
 814 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 93.0 °C
118000 psi
@Thickness 0.374 - 1.00 in,
Temperature 199 °F
 844 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 20.0 °C
122000 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 68.0 °F
 849 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 20.0 °C
123000 psi
@Thickness 0.374 - 1.00 in,
Temperature 68.0 °F
 864 MPa
@Thickness 12.7 mm,
Temperature 20.0 °C
125000 psi
@Thickness 0.500 in,
Temperature 68.0 °F
 887 MPa
@Thickness 1.45 mm,
Temperature 20.0 °C
129000 psi
@Thickness 0.0571 in,
Temperature 68.0 °F
Tensile Strength, Yield  52.0 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 1093 °C
7540 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1999 °F
0.2% offset
 61.0 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 1093 °C
8850 psi
@Thickness 0.374 - 1.00 in,
Temperature 1999 °F
0.2% offset
 110 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 982 °C
16000 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1800 °F
0.2% offset
 135 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 982 °C
19600 psi
@Thickness 0.374 - 1.00 in,
Temperature 1800 °F
0.2% offset
 218 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 871 °C
31600 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1600 °F
0.2% offset
 233 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 871 °C
33800 psi
@Thickness 0.374 - 1.00 in,
Temperature 1600 °F
0.2% offset
 271 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 760 °C
39300 psi
@Thickness 0.374 - 1.00 in,
Temperature 1400 °F
0.2% offset
 274 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 649 °C
39700 psi
@Thickness 0.374 - 1.00 in,
Temperature 1200 °F
0.2% offset
 283 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 538 °C
41000 psi
@Thickness 0.374 - 1.00 in,
Temperature 1000 °F
0.2% offset
 291 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 316 °C
42200 psi
@Thickness 0.374 - 1.00 in,
Temperature 601 °F
0.2% offset
 297 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 427 °C
43100 psi
@Thickness 0.374 - 1.00 in,
Temperature 801 °F
0.2% offset
 311 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 760 °C
45100 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1400 °F
0.2% offset
 322 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 649 °C
46700 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1200 °F
0.2% offset
 331 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 204 °C
48000 psi
@Thickness 0.374 - 1.00 in,
Temperature 399 °F
0.2% offset
 338 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 538 °C
49000 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 1000 °F
0.2% offset
 365 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 93.0 °C
52900 psi
@Thickness 0.374 - 1.00 in,
Temperature 199 °F
0.2% offset
 365 MPa
@Thickness 12.7 mm,
Temperature 20.0 °C
52900 psi
@Thickness 0.500 in,
Temperature 68.0 °F
0.2% offset
 383 MPa
@Thickness 9.50 - 25.4 mm,
Temperature 20.0 °C
55500 psi
@Thickness 0.374 - 1.00 in,
Temperature 68.0 °F
0.2% offset
 434 MPa
@Thickness 1.45 mm,
Temperature 20.0 °C
62900 psi
@Thickness 0.0571 in,
Temperature 68.0 °F
0.2% offset
 444 MPa
@Thickness 1.10 - 1.60 mm,
Temperature 20.0 °C
64400 psi
@Thickness 0.0433 - 0.0630 in,
Temperature 68.0 °F
0.2% offset
Elongation at Break  46 %
@Thickness 1.10 - 1.60 mm,
Temperature 982 °C
46 %
@Thickness 0.0433 - 0.0630 in,
Temperature 1800 °F
in 50.8 mm
 47 %
@Thickness 1.10 - 1.60 mm,
Temperature 871 °C
47 %
@Thickness 0.0433 - 0.0630 in,
Temperature 1600 °F
in 50.8 mm
 49 %
@Thickness 1.10 - 1.60 mm,
Temperature 20.0 °C
49 %
@Thickness 0.0433 - 0.0630 in,
Temperature 68.0 °F
in 50.8 mm
 50 %
@Thickness 1.10 - 1.60 mm,
Temperature 538 °C
50 %
@Thickness 0.0433 - 0.0630 in,
Temperature 1000 °F
in 50.8 mm
 54 %
@Thickness 12.7 mm,
Temperature 20.0 °C
54 %
@Thickness 0.500 in,
Temperature 68.0 °F
in 50.8 mm
 55 %
@Thickness 9.50 - 25.4 mm,
Temperature 20.0 °C
55 %
@Thickness 0.374 - 1.00 in,
Temperature 68.0 °F
in 50.8 mm
 56 %
@Thickness 1.10 - 1.60 mm,
Temperature 649 °C
56 %
@Thickness 0.0433 - 0.0630 in,
Temperature 1200 °F
in 50.8 mm
 57 %
@Thickness 9.50 - 25.4 mm,
Temperature 871 °C
57 %
@Thickness 0.374 - 1.00 in,
Temperature 1600 °F
in 50.8 mm
 58 %
@Thickness 1.45 mm,
Temperature 20.0 °C
58 %
@Thickness 0.0571 in,
Temperature 68.0 °F
in 50.8 mm
 59 %
@Thickness 9.50 - 25.4 mm,
Temperature 204 °C
59 %
@Thickness 0.374 - 1.00 in,
Temperature 399 °F
in 50.8 mm
 59 %
@Thickness 9.50 - 25.4 mm,
Temperature 649 °C
59 %
@Thickness 0.374 - 1.00 in,
Temperature 1200 °F
in 50.8 mm
 60 %
@Thickness 9.50 - 25.4 mm,
Temperature 93.0 °C
60 %
@Thickness 0.374 - 1.00 in,
Temperature 199 °F
in 50.8 mm
 61 %
@Thickness 9.50 - 25.4 mm,
Temperature 538 °C
61 %
@Thickness 0.374 - 1.00 in,
Temperature 1000 °F
in 50.8 mm
 62 %
@Thickness 9.50 - 25.4 mm,
Temperature 427 °C
62 %
@Thickness 0.374 - 1.00 in,
Temperature 801 °F
in 50.8 mm
 62 %
@Thickness 9.50 - 25.4 mm,
Temperature 982 °C
62 %
@Thickness 0.374 - 1.00 in,
Temperature 1800 °F
in 50.8 mm
 63 %
@Thickness 9.50 - 25.4 mm,
Temperature 316 °C
63 %
@Thickness 0.374 - 1.00 in,
Temperature 601 °F
in 50.8 mm
 69 %
@Thickness 9.50 - 25.4 mm,
Temperature 760 °C
69 %
@Thickness 0.374 - 1.00 in,
Temperature 1400 °F
in 50.8 mm
 69 %
@Thickness 9.50 - 25.4 mm,
Temperature 1093 °C
69 %
@Thickness 0.374 - 1.00 in,
Temperature 1999 °F
in 50.8 mm
 70 %
@Thickness 1.10 - 1.60 mm,
Temperature 760 °C
70 %
@Thickness 0.0433 - 0.0630 in,
Temperature 1400 °F
in 50.8 mm
 75 %
@Thickness 1.10 - 1.60 mm,
Temperature 1093 °C
75 %
@Thickness 0.0433 - 0.0630 in,
Temperature 1999 °F
in 50.8 mm
Modulus of Elasticity  132 GPa
@Temperature 1093 °C
19100 ksi
@Temperature 1999 °F
Heat treated at 1066°C, air cooled
 151 GPa
@Temperature 927 °C
21900 ksi
@Temperature 1700 °F
Heat treated at 1066°C, air cooled
 161 GPa
@Temperature 813 °C
23400 ksi
@Temperature 1500 °F
Heat treated at 1066°C, air cooled
 166 GPa
@Temperature 760 °C
24100 ksi
@Temperature 1400 °F
Heat treated at 1066°C, air cooled
 174 GPa
@Temperature 649 °C
25200 ksi
@Temperature 1200 °F
Heat treated at 1066°C, air cooled
 182 GPa
@Temperature 538 °C
26400 ksi
@Temperature 1000 °F
Heat treated at 1066°C, air cooled
 194 GPa
@Temperature 357 °C
28100 ksi
@Temperature 675 °F
Heat treated at 1066°C, air cooled
 212 GPa
@Temperature 24.0 °C
30700 ksi
@Temperature 75.2 °F
Charpy Impact 190 J140 ft-lbV Notch; solution heat-treated, not aged
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000128 ohm-cm
@Temperature 25.0 °C
0.000128 ohm-cm
@Temperature 77.0 °F
specimen aged 16000 hours at 650°C (1200°F)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 - 93.0 °C
6.39 µin/in-°F
@Temperature 68.0 - 199 °F
 12.2 µm/m-°C
@Temperature 20.0 - 204 °C
6.78 µin/in-°F
@Temperature 68.0 - 399 °F
 12.8 µm/m-°C
@Temperature 20.0 - 316 °C
7.11 µin/in-°F
@Temperature 68.0 - 601 °F
 13.1 µm/m-°C
@Temperature 20.0 - 427 °C
7.28 µin/in-°F
@Temperature 68.0 - 801 °F
 13.3 µm/m-°C
@Temperature 20.0 - 538 °C
7.39 µin/in-°F
@Temperature 68.0 - 1000 °F
 14.4 µm/m-°C
@Temperature 20.0 - 760 °C
8.00 µin/in-°F
@Temperature 68.0 - 1400 °F
 14.9 µm/m-°C
@Temperature 20.0 - 871 °C
8.28 µin/in-°F
@Temperature 68.0 - 1600 °F
 15.5 µm/m-°C
@Temperature 20.0 - 982 °C
8.61 µin/in-°F
@Temperature 68.0 - 1800 °F
 16.0 µm/m-°C
@Temperature 20.0 - 1093 °C
8.89 µin/in-°F
@Temperature 68.0 - 1999 °F
Specific Heat Capacity  0.398 J/g-°C
@Temperature 0.000 °C
0.0951 BTU/lb-°F
@Temperature 32.0 °F
 0.414 J/g-°C
@Temperature 50.0 °C
0.0989 BTU/lb-°F
@Temperature 122 °F
 0.440 J/g-°C
@Temperature 150 °C
0.105 BTU/lb-°F
@Temperature 302 °F
 0.456 J/g-°C
@Temperature 250 °C
0.109 BTU/lb-°F
@Temperature 482 °F
 0.473 J/g-°C
@Temperature 350 °C
0.113 BTU/lb-°F
@Temperature 662 °F
 0.481 J/g-°C
@Temperature 450 °C
0.115 BTU/lb-°F
@Temperature 842 °F
 0.494 J/g-°C
@Temperature 550 °C
0.118 BTU/lb-°F
@Temperature 1020 °F
 0.502 J/g-°C
@Temperature 650 °C
0.120 BTU/lb-°F
@Temperature 1200 °F
 0.590 J/g-°C
@Temperature 800 °C
0.141 BTU/lb-°F
@Temperature 1470 °F
 0.594 J/g-°C
@Temperature 850 °C
0.142 BTU/lb-°F
@Temperature 1560 °F
 0.594 J/g-°C
@Temperature 900 °C
0.142 BTU/lb-°F
@Temperature 1650 °F
 0.594 J/g-°C
@Temperature 700 °C
0.142 BTU/lb-°F
@Temperature 1290 °F
 0.594 J/g-°C
@Temperature 750 °C
0.142 BTU/lb-°F
@Temperature 1380 °F
 0.598 J/g-°C
@Temperature 950 °C
0.143 BTU/lb-°F
@Temperature 1740 °F
 0.598 J/g-°C
@Temperature 1000 °C
0.143 BTU/lb-°F
@Temperature 1830 °F
 0.598 J/g-°C
@Temperature 1050 °C
0.143 BTU/lb-°F
@Temperature 1920 °F
 0.603 J/g-°C
@Temperature 1100 °C
0.144 BTU/lb-°F
@Temperature 2010 °F
Thermal Conductivity  14.0 W/m-K
@Temperature 200 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 392 °F
 16.1 W/m-K
@Temperature 300 °C
112 BTU-in/hr-ft²-°F
@Temperature 572 °F
 17.9 W/m-K
@Temperature 400 °C
124 BTU-in/hr-ft²-°F
@Temperature 752 °F
 19.5 W/m-K
@Temperature 500 °C
135 BTU-in/hr-ft²-°F
@Temperature 932 °F
 21.0 W/m-K
@Temperature 600 °C
146 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 26.1 W/m-K
@Temperature 700 °C
181 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 26.1 W/m-K
@Temperature 800 °C
181 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 26.1 W/m-K
@Temperature 900 °C
181 BTU-in/hr-ft²-°F
@Temperature 1650 °F
 27.1 W/m-K
@Temperature 950 °C
188 BTU-in/hr-ft²-°F
@Temperature 1740 °F
 28.0 W/m-K
@Temperature 1000 °C
194 BTU-in/hr-ft²-°F
@Temperature 1830 °F
Melting Point 1335 - 1380 °C2435 - 2520 °F
Solidus 1335 °C2435 °F
Liquidus 1380 °C2520 °F
Maximum Service Temperature, Air 1093 °C1999 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.10 - 0.50 %0.10 - 0.50 %
Boron, B <= 0.015 %<= 0.015 %
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 14.5 - 17 %14.5 - 17 %
Cobalt, Co <= 2.0 %<= 2.0 %
Copper, Cu <= 0.35 %<= 0.35 %
Iron, Fe <= 3.0 %<= 3.0 %
Lanthanum, La 0.010 - 0.10 %0.010 - 0.10 %
Manganese, Mn 0.30 - 1.0 %0.30 - 1.0 %
Molybdenum, Mo 14 - 16.5 %14 - 16.5 %
Nickel, Ni 67 %67 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si 0.20 - 0.75 %0.20 - 0.75 %
Sulfur, S <= 0.015 %<= 0.015 %
Tungsten, W <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes Hastelloy® X alloy, sheet
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 16000 hours
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal
ATI Allegheny Ludlum Stainless Steel 334 (UNS S33400)

NHASAA / 16879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.