MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kennametal Stellite Hydroloy® HQ913®
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Proprietary stainless steel with low Co and Mn contents, formulated to resist cavitation and droplet impingement erosion.

Processing: Can be heat treated to increase ductility without affecting resistance to cavitation erosion. Work hardens easily; important to ensure good cutting action and to avoid rubbing during finishing operations. Easier to grind to final dimensions than the stainless steel it typically replaces.

Corrosion Resistance: Moderate. Resists mildly corrosive environments and slight abrasive conditions.

Applications: parts requiring cavitation or water droplet impingement erosion resistance such as hydraulic turbine runners or boiler feedwater pumps.

Forms: Castings, wrought specialty shapes, hardfacing, wire, and powder.

Product of former Deloro Stellite Inc. Similar to Ireca Alloy

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 274274Converted from Vickers hardness
Hardness, Knoop 306306Converted from Vickers hardness
Hardness, Rockwell C 3232
Hardness, Vickers 290290
Tensile Strength, Ultimate 862 MPa125000 psi
Tensile Strength, Yield 448 MPa65000 psi
Elongation at Break 35 %35 %
Reduction of Area 40 %40 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.20 %0.20 %
Chromium, Cr 17 %17 %
Cobalt, Co 9.0 %9.0 %
Iron, Fe 61.6 %61.6 %
Manganese, Mn 9.5 %9.5 %
Nitrogen, N 0.20 %0.20 %
Silicon, Si 2.5 %2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® STAR cast
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
Kennametal Stellite Delcrome® 93 White Cast Iron
Kennametal Stellite Delcrome® 90 White Cast Iron
Kennametal Stellite Nucalloy® 466 High-Silicon Nickel-Base Hardfacing Alloy

NSJNCA / 19194

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.