MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: High strength wrought Mg alloy used for high performance components, including at elevated temperature. Excellent corrosion resistance and easily machined. Can be extruded, forged and hot formed. Supplied in the T5 condition.

Key Words: AMS 2154 Class AA
Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.95 g/cc0.0704 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 110 - 118110 - 118
Tensile Strength  221 MPa
@Temperature 300 °C
32000 psi
@Temperature 572 °F
 393 MPa
@Temperature 200 °C
57000 psi
@Temperature 392 °F
 400 MPa
@Temperature 100 °C
58000 psi
@Temperature 212 °F
 407 MPa
@Temperature 20.0 °C
59000 psi
@Temperature 68.0 °F
Tensile Strength, Yield  124 MPa
@Strain 0.2 %,
Temperature 300 °C
18000 psi
@Strain 0.2 %,
Temperature 572 °F
 300 MPa
@Strain 0.2 %,
Temperature 100 °C
43500 psi
@Strain 0.2 %,
Temperature 212 °F
 300 MPa
@Strain 0.2 %,
Temperature 200 °C
43500 psi
@Strain 0.2 %,
Temperature 392 °F
 310 MPa
@Strain 0.2 %,
Temperature 20.0 °C
45000 psi
@Strain 0.2 %,
Temperature 68.0 °F
Elongation at Break 9.0 %9.0 %
Fatigue Strength 200 MPa
@# of Cycles 5.00e+7
29000 psi
@# of Cycles 5.00e+7
Axial; R = 0.1; Extruded Bar; ASTM E466
Fracture Toughness 16.0 MPa-m½14.6 ksi-in½KQ
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.4 µm/m-°C15.2 µin/in-°F
Thermal Conductivity 76.0 W/m-K527 BTU-in/hr-ft²-°F
 
Descriptive Properties
Corrosion Resistance10 - 40 MpyASTM B117 salt spray
Stress Corrosion CrackingPasses ASTM G44

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® ZK60A Magnesium Alloy, UNS M16600
Magnesium EA55RS-T4, Extruded
Magnesium EA65RS-T4, Extruded
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
SAE SiC/AZ91 Magnesium Matrix Composite, as cast

NMAGEL900 / 147649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.