System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Honeywell AClyn® 285P EAA copolymer
Categories:
Polymer
;
Thermoplastic
;
Ethylene Acrylic Acid
;
Ionomer
Material Notes:
Ionomer of an EAA copolymer, based on AC 5120, which is 80% neutralized with Sodium, as is soluble in water. The sodium provides water sensitivity. This product can be used in temporary protective coatings.
Information provided by Honeywell
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Brookfield Viscosity
30000
cP
@Temperature 190 °C
30000
cP
@Temperature 374 °F
Chemical Properties
Metric
English
Comments
Total Acid Number
20
20
Thermal Properties
Metric
English
Comments
Dropping Point
82.0
°C
180
°F
Mettler
Descriptive Properties
Hardness
1 dmm
ASTM D5
Product Form
Granule
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Honeywell AClyn® 246 EAA copolymer
Honeywell A-C® 5120 EAA copolymer
Honeywell AClyn® 201 EAA copolymer
Honeywell AClyn® 201A EAA copolymer
Honeywell AClyn® 295A EAA copolymer
PHONWL088 / 179633
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.