MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petromont 2001 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 2001 is a high-density polyethylene copolymer resin produced using the UNIPOL ® Process. This resin has been designed specifically for film for various applications such as notion and millinery bags, food packaging, "T-shirt" bags, industrial and agricultural bags, etc.

Petromont HDPE 2001 has a broad molecular weight distribution. This, combined with its high molecular weight and balanced density, results in excellent performance at high extrusion rates with high film strength and rigidity. The excellent draw down characteristics permit production of high quality thin films. This product consists of an improved formulation.

Key Words: Film
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D1505
Melt Flow 0.070 g/10 min0.070 g/10 minI2; ASTM D1238
 10 g/10 min10 g/10 minI21; ASTM D238
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FPetromont
Vicat Softening Point 124 °C255 °FASTM D1525
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stanelco Bioplast® GS 2189 Biodegradable Plastic
SCG Chemicals EL-Lene™ H6670B High Density Polyethylene Film
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin
LG Chemical SEETEC PH150 HDPE Blown Film Grade

PPETROM07 / 56201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.