MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tin-Bearing Copper Nickel, UNS C72500, Extra Hard flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent corrosion resistance. Excellent hot and cold formability. Fabricated by blanking, brazing, coining, drawing, etching, forming and bending, heading and upsetting, roll threading and knurling, shearing, spinning, squeezing, stamping and swaging.

Applications: relay and switch springs, connectors, brazing alloy, lead frames, control and sensing bellows.

Test specimen: flat products - 1mm thickness.

Key Words: Cupronickel with Tin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8888
Tensile Strength, Ultimate 600 MPa87000 psi
Tensile Strength, Yield  555 MPa
@Strain 0.5 %
80500 psi
@Strain 0.5 %
 590 MPa
@Strain 0.2 %
85600 psi
@Strain 0.2 %
Elongation at Break 2.0 %2.0 %In 50 mm
Modulus of Elasticity 137 GPa19900 ksi
Poissons Ratio 0.320.32Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 52.0 GPa7540 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000157 ohm-cm0.0000157 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.5 µm/m-°C
@Temperature 20.0 - 300 °C
9.17 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 55.0 W/m-K
@Temperature 20.0 °C
382 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1060 - 1130 °C1940 - 2070 °F
Solidus 1060 °C1940 °F
Liquidus 1130 °C2070 °F
Annealing Point 649 - 801.7 °C1200 - 1475 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 650 - 800 °C1200 - 1470 °F
Hot-Working Temperature 850 - 950 °C1560 - 1740 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 88.2 %88.2 %
Iron, Fe <= 0.60 %<= 0.60 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn <= 0.20 %<= 0.20 %
Nickel, Ni 8.5 - 10.5 %8.5 - 10.5 %
Other, total <= 0.20 %<= 0.20 %
Tin, Sn 1.8 - 2.8 %1.8 - 2.8 %
Zinc, Zn <= 0.50 %<= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tin-Bearing Copper Nickel, UNS C72500, Quarter Hard flat products
Copper Nickel Tin, UNS C72800
Tin-Bearing Copper Nickel, UNS C72500, Annealed wire
Tin-Bearing Copper Nickel, UNS C72500, Half Hard flat products
Tin-Bearing Copper Nickel, UNS C72500, Hard flat products

MC72500b6 / 11767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.