MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baytec® ENC-140P Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Baytec ENC-140P is an epoxy-modified polypropylene oxide-based triol.

Properties / Applications: Baytec ENC-140P is an epoxy-modified polypropylene oxide-based triol. It is used as the hydroxy co-reactant in the production of hard, tough polyurethane elastomers with excellent long-term high-temperature resistance. With Baytec ENC 88 isocyanate, a rigid elastomer is obtained that is capable of withstanding a temperature of 140°C for an extended period of time. Other polyisocyanates or isocyanate-terminated prepolymers may also be employed to produce solid elastomers of varying hardness with good temperature resistance. To ensure good elastomer properties, mix ratios of isocyanate to Baytec ENC-140P polyol should be such that an index of 1.44 is maintained. Amine catalysts, such as Desmorapid® DB, may be employed with or without tin catalysts, but should be added to the Baytec ENC-140P polyol only at the time of casting. Typical applications include the encapsulation of electrical components, including those subjected to extreme heat. As with any product, use of Baytec ENC-140P polyol in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Bulk Density 1.08 g/cc0.0390 lb/in³
Viscosity 1350 cP1350 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 227 °C441 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.25 %<= 0.25 %
 
Descriptive Properties
AppearancePale yellow to pale amber viscous liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro MONDUR® 1453 Polyurethane
BCC Products BC 8165 Urethane Casting
BCC Products BC 8782 Urethane Casting
BCC Products Kwik Kast BC 8001 Urethane Casting
BCC Products Kwik Kast BC 8002 Urethane Casting

PCOVEST0241 / 202024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.