MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron MasterMold 12-3 Flexible Mold Making Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Master mold 12-3 is formulated for versatility, high elasticity and strength. It is a 2-component polyurethane system and can be easily spread on any model to produce a smooth bubble-free mold surface which captures the finest details. Its elasticity, softness and high tear strength permit easy peeling from intricate and undercut shapes. At the same time, its unique dimensional memory permits casting molds without any exterior support in numerous instances. For example, a mold can be removed from a totally enveloped shape, such as a table leg, by cutting one side with a knife. Then the mold can be held together with rubber bands or simple fasteners for casting.

Processing:

Part A Resin: Blue, no-slump thixotropic paste, 8.6 lbs/gal

Part B Converter: Yellow, no-slump thixotropic paste, 11.2 lbs/gal

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838
Tensile Strength at Break 1.24 MPa180 psi
Elongation at Break >= 600 %>= 600 %
 
Processing PropertiesMetricEnglishComments
Dry Time 8 - 12 hour8 - 12 hourHard
Working Life 60 - 90 min60 - 90 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive
AorTech Biomaterials ECSil™ 90A Biomedical Carbonate Silicone Pellets
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer

PABKW018 / 22059

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.