MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 40 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
Categories: Polymer; Thermoset; Silicone

Material Notes: QSil 40 is a general purpose two-part, room temperature, condensation cure siloxane elastomer. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section Catalyst by weight. Cure speed can be accelerated by adding DBT catalyst in increments of 0.1%. This will not alter the physical properties of the material. QSil 40 exhibits excellent release properties. However, strong adhesion can be achieved through the use of a primer.

Key Features:

  • Good adhesion with use of a primer
  • Self-leveling
  • Variable cure speed
Part of the Amber Chemical Group. Data provided by manufacturer

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccUncatalyzed, DBT Catalyst
 1.20 g/cc1.20 g/cc"A" component
 1.47 g/cc1.47 g/ccUncatalyzed, Deep Section Catalyst
Viscosity 6500 cP6500 cPUncatalyzed, Deep Section Catalyst
 11000 cP11000 cP
Storage Temperature 4.00 °C39.2 °F12 months
 5.00 - 27.0 °C41.0 - 80.6 °F3 months
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength 1.38 MPa200 psi
Elongation at Break 200 %200 %
Tear Strength 3.51 kN/m20.0 pli
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 120 min2.00 hourCatalyzed, Deep Section Catalyst
 240 min4.00 hourcatalyzed, DBT Catalyst
Gel Time 45.0 min45.0 mincatalyzed, DBT Catalyst
 70.0 min70.0 mincatalyzed, Deep Section Catalyst
 
Descriptive Properties
ColorWhite
Hegman Grind3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 551 QSI Quantum Silicones Silicone Potting Material
CHT Group QSil 553 QSI Quantum Silicones Silicone Potting Material
Mid-Mountain Materials ARMATEX® SRS 40 Silica Fabric Impregnated with Silicone Rubber
CHT Group QLE 1039 QSI Quantum Silicones 40 Durometer Addition Cure Elastomer for Coating
CHT Group QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material

PACC037 / 22164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.