MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

American Basswood Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Hardwood. Easy to work with hand tools. Fair planing, poor shaping, poor steam bending. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Permeable
Common Applications: Constructional veneer, turnery, piano keys, woodware

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Tilia americana; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³Oven Dry Weight/Unseasoned Volume
 0.657 g/cc0.0237 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1100 N247 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1200 N270 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1800 N405 lb (f)Side
Tensile Strength, Ultimate 1.93 MPa280 psiPerpendicular to Grain*
 2.40 MPa348 psiPerpendicular to Grain
Modulus of Rupture 0.0345 GPa5.00 ksiStatic Bending*
 0.0600 GPa8.70 ksiIn Bending
Flexural Yield Strength 18.6 MPa2700 psiFiber Stress at Elastic Limit; Static Bending*
 40.7 MPa5900 psiBending stress at proportional limit
Flexural Modulus 7.10 GPa1030 ksiStatic Bending*
 10.1 - 10.3 GPa1460 - 1490 ksiIn Bending
Compressive Strength 1.45 MPa210 psiPerpendicular to Grain*
 2.60 MPa377 psiPerpendicular to Grain
 11.8 MPa1710 psiParallel to Grain*
 15.2 MPa2210 psiMax Crushing Strength Parallel to Grain*
 32.4 - 33.0 MPa4700 - 4790 psiParallel to Grain
Poissons Ratio 0.0220.022µTL, 12% Moisture Content
 0.0340.034µRL, 12% Moisture Content
 0.3460.346µTR, 12% Moisture Content
 0.3640.364µLR, 12% Moisture Content
 0.4060.406µLT, 12% Moisture Content
 0.9120.912µRT, 12% Moisture Content
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 4.21 MPa610 psiParallel to Grain*
 6.80 MPa986 psiOrientation Unknown
Impact 2.02.0in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 62006200psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00290 J/cm³0.420 in-lb/in³Static Bending*
Work to Maximum Load 0.0359 J/cm³5.20 in-lb/in³Static Bending*
Cleavage 23.0 kN/m131 lb/inRadial surface of failure, Unseasoned*
 29.0 kN/m165 lb/inTangential surface of failure, Unseasoned*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0922 W/m-K0.640 BTU-in/hr-ft²-°FOven Dry
 0.111 W/m-K0.770 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 6.6 %6.6 %Radial; Green to Zero Moisture
 9.3 %9.3 %Tangential; Green to Zero Moisture
 15.8 %15.8 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorCreamy white to pale brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products MB 1300 Polyurethane Foam Modeling Board
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
American Balsa Wood
DIAB ProBalsa® PB Standard Balsa Wood
American Beech Wood

PTSAN / 71297

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.