MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: Mill Hardened
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%
Stress Relaxation after 1000 hrs @ 200°C: 76%
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2
Formability Ratio (bad Way): 5
Superficial Hardness: 30T 79-30N 48

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-768
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 95 - 10295 - 102
Hardness, Vickers 210 - 278210 - 278
Tensile Strength, Ultimate 750 - 900 MPa109000 - 131000 psi
Tensile Strength, Yield 650 - 870 MPa94300 - 126000 psi
Elongation at Break 7.0 - 17 %7.0 - 17 %
Modulus of Elasticity 138 GPa20000 ksi
Fatigue Strength 280 - 310 MPa
@# of Cycles 1.00e+8
40600 - 45000 psi
@# of Cycles 1.00e+8
Reverse Bending (R=1)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000290 - 0.00000380 ohm-cm0.00000290 - 0.00000380 ohm-cm45-60% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.0 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 230 W/m-K1600 BTU-in/hr-ft²-°F
Melting Point 1030 - 1070 °C1890 - 1960 °F
Solidus 1030 °C1890 °F
Liquidus 1070 °C1960 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.15 - 0.50 %0.15 - 0.50 %
Cobalt, Co 0.35 - 0.60 %0.35 - 0.60 %
Copper, Cu 99 %99 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy 174 Strip; 1/2HT (TH02) Temper (UNS C17410)
Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200)
Materion Alloy 10X CuCoBeZr Alloy, TH04 Temper
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17500)
Materion Brush 60™ 3/4 HT

NBB484 / 15192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.