MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Laponite® S485 Magnesium Aluminum Silicate
Categories: Ceramic; Clay

Material Notes: Description: Laponite S482 is a modified synthetic magnesium aluminum silicate with pronounced platelet structure. When dispersed in water, Laponite S482 forms a transparent, pourable liquid up to a concentration of 25% solids. In resin formulations, however, significant thixotropy and a high yield value can be incorporated.

Application:

  • Emulsion paints
  • Putties
  • Adhesives
  • Ceramic frits / glazes / slips
  • Grinding pastes and abrasives
  • Silicon resin based external paints
  • Artist paints / finger paints
  • Water reducible systems

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.50 g/cc0.0903 lb/in³
Brightness 80 %80 %Elrepho R 457
Particle Mesh Size >= 325 Mesh>= 325 Mesh95%
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 400 °C752 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 15 %<= 15 %
 
Descriptive Properties
Color/FormFree flowing white powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Laponite® S Synthetic Layered Fluorosilicate
BYK Laponite® RDS Synthetic Layered Silicate
BYK Laponite® RD Synthetic Layered Silicate
BYK Laponite® OG Clay Additive
BYK Laponite® LV Clay Additive

PBYK069 / 185066

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.