MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemours Teflon® PTFE Grade B Filter Fabric Finish  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Teflon® PTFE B is an aqueous dispersion containing approximately 61%, by total weight, of active ingredients, which include 0.05 to 0.5 mm polytetrafluoroethylene (PTFE) resin particles. It is a milky white liquid with a pH of 8.5.

Compared with other grades of PTFE dispersions, Teflon® PTFE B is a special formulation designed for application to woven glass fabric used to make bags for difficult gaseous filtration or product collection systems. The bags must be self-lubricating and resist clogging for years, while being flexed in high-temperature, corrosive atmospheres.

When properly applied, Teflon® PTFE B improves the flex life, heat and chemical resistance, and antiadhesion behavior of glass fabric, resulting in filter bags with enhanced service life and efficiency.

Applications

Large, high-performance filter bags are made of woven glass fabric treated with Teflon® PTFE B. Principal markets are for pollution control of coal-fired boilers in utility and industrial plants, and for product collection in hostile environments, such as those for producing carbon black.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Polytetrafluoroethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D4441
Solids Content 61 %61 %Percent of PTFE resin solids; ASTM D4441
Particle Size 0.22 µm0.22 µmAverage dispersion particle size
pH 8.58.5ASTM E70
 
Thermal PropertiesMetricEnglishComments
Melting Point 327 °C621 °FASTM D1457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Chemours Teflon® PTFE 8A Granular Molding Powder
Chemours Teflon® PTFE 67 Resin for Lubricated Paste Extrusion
Chemours Teflon® C PFA Grade 510 Static Dissipating Semiconductive Resin
Chemours Teflon® FEP 121A Aqueous Dispersion

PDU9207 / 33326

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.