MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Polikim KESTAMID® PA6G Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical properties. It is replacing aluminum, copper, bronze, steel, fiber, brass and other metals in many applications with superior advantages. It is cheaper, lighter, harder and more durable than these metals. In terms of cost, Kestamid® is 1/7th of bronze, 1/5th of copper and 1/3rd of brass. As its density is low, purchase and delivery costs become less. Using Kestamid® instead of metal components helps push selling price and delivery cost down. It contributes significantly to the final producer in reducing costs and increasing market share. As it does not require lubrication, maintenance costs are also reduced to a minimum. High wear and impact resistances make Kestamid® durable. Taking its operational life into consideration, the advantages and superiorities of Kestamid® compared to the above-mentioned metals become even more obvious. Kestamid® is a “fix and forget” type of material. It is possible to produce steel bush core gears, pulleys and mixer fans or produce cylinders with steel axis by making use of techniques specific to the production of Kestamid® combined with the mechanical resistance of metals.

Information provided by Polikim Polimer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption at Saturation 7.0 %7.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484ISO 868
Tensile Strength, Ultimate 83.4 MPa12100 psiISO 527
Elongation at Break >= 20 %>= 20 %ISO 527
Tensile Modulus 4.00 GPa580 ksiISO 527
Compressive Strength 93.2 MPa13500 psiISO 604
Compressive Modulus 2.70 GPa392 ksiISO 604
Izod Impact, Notched (ISO) 5.60 kJ/m²2.66 ft-lb/in²ISO 180
Charpy Impact Unnotched NBNBISO 179
Coefficient of Friction 0.390.39
K Factor (Wear Factor) 0.440.44[mg/km]
K (wear) Factor 500 x 10-8 mm³/N-M248 x 10-10 in³-min/ft-lb-hr
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmISO 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmISO 60093
Dielectric Constant 3.73.7ISO 60250
Dielectric Strength 25.0 kV/mm635 kV/inISO 50243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 110 °C230 °Fcontinuous
 170 °C338 °Fshort term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GEHR Plastics PA 6 G Nylon 6, Cast, Dry
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled
Polikim KESTAMID® HS Polyamide 6, Heat Resistant
Aluminum 1060-H16
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide

PPOLIK011 / 99821

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.