MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lanxess Addocat® 117 PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Addocat 117 is an excellent co-catalyst for all polyurethane systems. Addocat 117 is especially suited to be used as co-catalyst for the reduced odor catalysis of flexible polyester slabstock in combination with urea, Addocat DMEA and Addocat SO.

Function: Co-catalyst for polyurethanes, specially for low odor polyester flexible slabstock foam.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.850 g/cc0.0307 lb/in³
Water Absorption <= 0.50 %<= 0.50 %
Viscosity 1.0 cP1.0 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 130 °C266 °FInitial
Pour Point -18.3 °C-1.00 °F
Flash Point 21.0 °C69.8 °FDIN 51755
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearancecolorless to yellowish liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Addocat® 109 PU Catalyst/Activator
Lanxess Addocat® 108 PU Catalyst/Activator
Lanxess Addocat® 105 PU Catalyst/Activator
Lanxess Addovate® EM PU Additive
Struktol STRUKSILON 8002 Silicone Stabilizer for PU-Rigid Foam

PLANY8184 / 208577

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.