MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Bicor® 420 HS OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor HS is a two-side coated, sealable OPP film designed for general use in overwrap and horizontal packaging. This film is suitable as an unsupported web or lamination. It can be surface printed, or used unprinted.

Availability: Latin America, North America and South America

Key Features:

  • Outstanding optical properties
  • Robust machinablity
  • Low and consistent COF
  • Excellent hot slip
  • Excellent flavor and aroma barrier
  • Printable on both sides
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
  • In Lamination Lap Sealable
Applications:
  • Biscuits/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Gum
  • Confectionery, Sugar
Uses:
  • Box Overwrap Flexible Packaging
  • HFF Flexible Packaging
  • Pre-made Bags - Flexible Packaging
  • Tobacco Overwrap Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 7.60 g/m²/day
@Temperature 38.0 °C
0.489 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 17.8 microns0.700 milNominal; ExxonMobil Method
Coating Weight 16.5 g/m²10.3 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.220.22ExxonMobil Method
Film Tensile Strength at Break, MD 138 MPa20000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 228 MPa33000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 4.5 %
@Temperature 135 °C
4.5 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 4.5 %
@Temperature 135 °C
4.5 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 1.5 %1.5 %ExxonMobil Method
Gloss 90 %90 %45º; ExxonMobil Method
 
Descriptive Properties
Crimp Seal MST182°F
Crimp Seal Strength540 g/in260°F, 20psi, 3/4sec
Yield42000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ipiranga Petrochem PH 0361 Polypropylene
Ipiranga Petrochem PH 0950 Polypropylene
ExxonMobil PP4712E1 Polymer Grade for Oriented Film
ExxonMobil Bicor® 84 AOH OPP Film
Epsilon Polymers XJ-015 Polypropylene

PEXB395 / 37700

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.