MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay ALKAMIDE® DC-212/S Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: A liquid coconut derived super diethanolamide (85%) comonly used in the preparation of high foaming cosmetic products.1:1 Coconut DEA 85% solids. Economical foam booster and viscosifier. Used in hand dishwash liquids and household and institutional cleaners.

Chemical Name: COCAMIDE DEA

CAS: 68603-42-9, 111-42-2, 111-42-2

Available in: Asia Pacific, Europe, Latin America and North America

Applications: The excellent performance boosting properties displayed by ALKAMIDE DC 212/S make it an ideal additive in the preparation of a wide variety of formulated products. Typical systems that incorporate ALKAMIDE DC 212/S include shampoos, hand soaps, facial scrubs, bubble baths, liquid dishwash, and assorted light duty and heavy duty cleaners. ALKAMIDE DC 212/S is also an excellent viscosity building agent for formulated systems. At relatively low concentration levels it markedly improves the viscosity effectiveness of most anionic surfactants.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 9.0 - 10.59.0 - 10.51% Solution; RP-0420
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 1.0<= 1.0[mg KOH/g]; RP-0008
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 4.0<= 4.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %Karl Fisher; RP-0321
 
Descriptive Properties
AppearanceClean, clear liquidRP-0064
CompositionAmide Content>84.5%, CALC
 Ester<7.0%, RP-0176
 Total Alkalinity as DEA<6.0%, EQ.WT. 105, RP-0040

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LKAB Minerals Reclaimed Firebrick
LKAB Minerals Reclaimed Corderite

WRHOD022 / 137252

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.