MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Michem® Prime 4983-40R Ethylene acrylic acid dispersion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Description: Ethylene acrylic acid dispersion

Usage: Michem® Prime 498340R is a high solids, more economical version of Michem® Prime 4983R. Like Michem® Prime 4983R, this product provides outstanding adhesion to metallic and cellulosic substrates and enhances the water, grease, oil and solvent resistance of coatings and adhesives. The adhesion properties of Michem® Prime facilitate its use as a primer for extrusion coatings. Utilizing this "tie coat" functionality, dissimilar materials can be combined to produce a substrate with the unique properties of each material.

When manufactured in the USA product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1 (Restricted) and Commission Regulation (EU) n° 10/2011(Restricted)
Germany: BfR Recommendation XIV (Restricted)and BfR Recommendation XXXVI (Restricted)

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives.
175.300: Resinous and polymeric components of coatings. (Restricted)
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 - 0.990 g/cc0.970 - 0.990 g/cc
Volatiles 59 - 61 %59 - 61 %
pH >= 7.0>= 7.0Recommended pH of system
 7.4 - 8.47.4 - 8.4
Brookfield Viscosity 1000 - 4000 cP1000 - 4000 cPSpindle # 3, rpm 30
 
Descriptive Properties
AppearanceWhite, viscous liquid
Emulsifier ChargeAmmoniated dispersion
Solids TypeEthylene Acrylic Acid Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® Michem® Prime 4990R Ethylene acrylic acid dispersion
Michelman® Michem® Prime 4983R Ethylene acrylic acid dispersion
Michelman® Michem® Prime 2960 Ethylene acrylic acid dispersion

WMICHEL160 / 135077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.