| Physical Properties | Metric | English | Comments |
|---|
| Density | 7.872 g/cc | 0.2844 lb/in³ |
| |
| Mechanical Properties | Metric | English | Comments |
|---|
| Tensile Strength, Ultimate | 303 - 358 MPa | 43900 - 51900 psi |
| Tensile Strength, Yield | 180 - 240 MPa | 26100 - 34800 psi |
| Elongation at Break | 42 - 48 % | 42 - 48 % |
| Modulus of Elasticity | 200 GPa | 29000 ksi |
| Bulk Modulus | 160 GPa | 23200 ksi |
| Poissons Ratio | 0.29 | 0.29 |
| Machinability | 55 % | 55 % |
| Shear Modulus | 80.0 GPa | 11600 ksi |
| |
| Electrical Properties | Metric | English | Comments |
|---|
Electrical Resistivity | 0.0000142 ohm-cm @Temperature 20.0 °C | 0.0000142 ohm-cm @Temperature 68.0 °F |
| | 0.0000190 ohm-cm @Temperature 100 °C | 0.0000190 ohm-cm @Temperature 212 °F |
| | 0.0000263 ohm-cm @Temperature 200 °C | 0.0000263 ohm-cm @Temperature 392 °F |
| | 0.0000458 ohm-cm @Temperature 400 °C | 0.0000458 ohm-cm @Temperature 752 °F |
| | 0.0000734 ohm-cm @Temperature 600 °C | 0.0000734 ohm-cm @Temperature 1110 °F |
| | 0.0000905 ohm-cm @Temperature 700 °C | 0.0000905 ohm-cm @Temperature 1290 °F |
| | 0.0001081 ohm-cm @Temperature 800 °C | 0.0001081 ohm-cm @Temperature 1470 °F |
| | 0.000113 ohm-cm @Temperature 900 °C | 0.000113 ohm-cm @Temperature 1650 °F |
| | 0.0001165 ohm-cm @Temperature 1000 °C | 0.0001165 ohm-cm @Temperature 1830 °F |
| | 0.0001193 ohm-cm @Temperature 1100 °C | 0.0001193 ohm-cm @Temperature 2010 °F |
| | 0.0001216 ohm-cm @Temperature 1200 °C | 0.0001216 ohm-cm @Temperature 2190 °F |
| |
| Thermal Properties | Metric | English | Comments |
|---|
CTE, linear | 12.6 µm/m-°C @Temperature 0.000 - 100 °C | 7.00 µin/in-°F @Temperature 32.0 - 212 °F |
| | 13.1 µm/m-°C @Temperature 0.000 - 200 °C | 7.28 µin/in-°F @Temperature 32.0 - 392 °F |
| | 13.5 µm/m-°C @Temperature 0.000 - 300 °C | 7.50 µin/in-°F @Temperature 32.0 - 572 °F |
| | 13.7 µm/m-°C @Temperature 0.000 - 400 °C | 7.61 µin/in-°F @Temperature 32.0 - 752 °F |
| | 13.7 µm/m-°C @Temperature 0.000 - 1000 °C | 7.61 µin/in-°F @Temperature 32.0 - 1830 °F |
| | 14.2 µm/m-°C @Temperature 0.000 - 500 °C | 7.89 µin/in-°F @Temperature 32.0 - 932 °F |
| | 14.6 µm/m-°C @Temperature 0.000 - 600 °C | 8.11 µin/in-°F @Temperature 32.0 - 1110 °F |
| | 14.9 µm/m-°C @Temperature 0.000 - 700 °C | 8.28 µin/in-°F @Temperature 32.0 - 1290 °F |
| | 16.6 µm/m-°C @Temperature 0.000 - 800 °C | 9.22 µin/in-°F @Temperature 32.0 - 1470 °F |
Specific Heat Capacity | 0.481 J/g-°C @Temperature >=100 °C | 0.115 BTU/lb-°F @Temperature >=212 °F |
| | 0.519 J/g-°C @Temperature 150 - 200 °C | 0.124 BTU/lb-°F @Temperature 302 - 392 °F |
| | 0.536 J/g-°C @Temperature 200 - 250 °C | 0.128 BTU/lb-°F @Temperature 392 - 482 °F |
| | 0.553 J/g-°C @Temperature 250 - 300 °C | 0.132 BTU/lb-°F @Temperature 482 - 572 °F |
| | 0.595 J/g-°C @Temperature 350 - 400 °C | 0.142 BTU/lb-°F @Temperature 662 - 752 °F |
| | 0.662 J/g-°C @Temperature 450 - 500 °C | 0.158 BTU/lb-°F @Temperature 842 - 932 °F |
| | 0.754 J/g-°C @Temperature 550 - 600 °C | 0.180 BTU/lb-°F @Temperature 1020 - 1110 °F |
| | 0.846 J/g-°C @Temperature 850 - 900 °C | 0.202 BTU/lb-°F @Temperature 1560 - 1650 °F |
| | 0.867 J/g-°C @Temperature 650 - 700 °C | 0.207 BTU/lb-°F @Temperature 1200 - 1290 °F |
| | 1.105 J/g-°C @Temperature 700 - 750 °C | 0.2641 BTU/lb-°F @Temperature 1290 - 1380 °F |
Thermal Conductivity | 27.3 W/m-K @Temperature 1000 °C | 189 BTU-in/hr-ft²-°F @Temperature 1830 °F |
| | 28.4 W/m-K @Temperature 800 °C | 197 BTU-in/hr-ft²-°F @Temperature 1470 °F |
| | 36.3 W/m-K @Temperature 600 °C | 252 BTU-in/hr-ft²-°F @Temperature 1110 °F |
| | 45.2 W/m-K @Temperature 400 °C | 314 BTU-in/hr-ft²-°F @Temperature 752 °F |
| | 54.7 W/m-K @Temperature 200 °C | 380 BTU-in/hr-ft²-°F @Temperature 392 °F |
| | 60.2 W/m-K @Temperature 100 °C | 418 BTU-in/hr-ft²-°F @Temperature 212 °F |
| | 65.2 W/m-K @Temperature 0.000 °C | 452 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
| Melting Point | 1426 °C | 2599 °F |
| |
| Component Elements Properties | Metric | English | Comments |
|---|
| Carbon, C | <= 0.10 % | <= 0.10 % |
| Iron, Fe | 99.31 - 99.7 % | 99.31 - 99.7 % |
| Manganese, Mn | 0.30 - 0.50 % | 0.30 - 0.50 % |
| Phosphorus, P | <= 0.040 % | <= 0.040 % |
| Sulfur, S | <= 0.050 % | <= 0.050 % |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.