MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM)  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Key Features:
  • Unfilled
  • High impact or high impact modified
  • Light stabilized or stable to light
  • Heat stabilized or stable to heat

Suitable processing methods:

  • Injection molding

Triax® is now a INEOS Styrolution trade name; this grade is discontinued. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³
Melt Density 0.900 g/cc
@Temperature 260 °C
0.0325 lb/in³
@Temperature 500 °F
Water Absorption 6.0 %6.0 %
Moisture Absorption at Equilibrium 1.7 %1.7 %23°C/50% R.H.
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psi
Elongation at Break >= 50 %>= 50 %Nominal
Elongation at Yield 3.2 %3.2 %
Tensile Modulus 1.90 GPa276 ksi
Charpy Impact Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Charpy Impact, Notched 7.40 J/cm²35.2 ft-lb/in²
 1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
Puncture Energy 40.0 J29.5 ft-lbPuncture energy +23°C
 40.0 J29.5 ft-lbPuncture energy -30°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
Dielectric Strength 34.0 kV/mm864 kV/in
Dissipation Factor  0.029
@Frequency 100 Hz
0.029
@Frequency 100 Hz
 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 105 µm/m-°C
@Temperature 20.0 °C
58.3 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 115 µm/m-°C
@Temperature 20.0 °C
63.9 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 2.20 J/g-°C0.526 BTU/lb-°FMelt
Thermal Conductivity 0.145 W/m-K1.01 BTU-in/hr-ft²-°FMelt
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °F
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °F
Vicat Softening Point 102 °C216 °F50°C/h 50N
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding
Mold Temperature 80.0 °C176 °FInjection Molding
Ejection Temperature 90.0 °C194 °F
Injection Velocity 40.0 mm/sec1.57 in/sec
 
Descriptive Properties
Effective thermal diffusivity0.732E-7 m²/sMelt

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Dry)
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned)
INEOS Styrolution Terblend® N NM-19 ABS/PA6 (Dry)
INEOS Styrolution Triax® 1315 GF ABS + Polyamide Blend (DAM)
Daicel CEVIAN® A1700 PA/ABS Alloy, DAM

PB10338 / 26376

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.