MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The combination of mineral and glass fibers result in a high performance, low warp and cost effective engineering thermoplastic. It exhibits high strength, good UV resistance, rigidity and good heat distortion temperatures. It has a relatively high resistance to creep under load. The heat stabilizer system extends its retention of properties at elevated temperatures. It has good chemical resistance to greases, oils and hydrocarbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Water Absorption 0.90 %0.90 %24 hour; ISO Test
 5.7 %5.7 %ISO 62
Moisture Absorption at Equilibrium 1.6 %1.6 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM Test
Tensile Strength at Break 120 MPa17400 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 118 MPa17100 psi5mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5mm/min; ISO 527
 2.0 %2.0 %0.2 in/min; ASTM Test
Tensile Modulus 8.40 GPa1220 ksi1mm/min; ISO 527
Flexural Strength 170 MPa24700 psiISO Data
 190 MPa27600 psiASTM Test
Flexural Modulus 7.16 GPa1040 ksiASTM Test
 7.30 GPa1060 ksiISO Data
Izod Impact, Notched 0.550 J/cm
@Thickness 3.17 mm
1.03 ft-lb/in
@Thickness 0.125 in
ASTM Test
Charpy Impact Unnotched 4.40 J/cm²20.9 ft-lb/in²ISO 179
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 31.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
17.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75
Flammability, UL94 HBHB
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
ColorBK-106A
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ TX1001 Copolyester
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Conditioned)
Envalior Durethan® BKV 30 G H2.0 900051 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)

PBASF9195 / 84959

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.