MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior Durethan® KU 2-2184/15 H3.0 000000 Nylon 6 (PA6), 65% Glass/Mineral Reinforced, Flame Retardant, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant; Nylon 6, Glass/Mineral Reinforced

Material Notes: 65% glass fibers and mineral, UL94V-0 (1.2 mm)

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.2 %1.2 %50% RH; IOS 62
Water Absorption at Saturation 3.5 %3.5 %IOS 62
Linear Mold Shrinkage, Flow 0.0031 cm/cm0.0031 in/in60x60x2; ISO 2577
 0.0032 cm/cm0.0032 in/in150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse 0.0043 cm/cm0.0043 in/in60x60x2; ISO 2577
 0.0070 cm/cm0.0070 in/in150x105x3; ISO 2577
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
5.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 190 MPa27600 psiISO 2093-1
Tensile Strength at Break 75.0 MPa10900 psi5 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1,-2
Tensile Modulus 5.80 GPa841 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 110 MPa16000 psi2 mm/min; ISO 178-A
Flexural Modulus 6.70 GPa972 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 2.0 %2.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -40.0 °C
<= 4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched 1.50 J/cm²7.14 ft-lb/in²
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 <= 1.00 J/cm²
@Temperature -40.0 °C
<= 4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 180-1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
IEC 60250
 7.1
@Frequency 100 Hz
7.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
@Thickness 1.00 mm
711 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.035
@Frequency 1e+6 Hz
0.035
@Frequency 1e+6 Hz
IEC 60250
 0.11
@Frequency 100 Hz
0.11
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °F
Mold Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® DP BM 65 X FM30 901510 Nylon 6 (PA6), 65% Mineral/Glass Fiber Reinforced, Dry

PLANW9584 / 208375

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.