MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Indium Corp. Indalloy® 171 Pb-Sn Solder Alloy
Categories: Metal; Nonferrous Metal; Lead Alloy; Solder/Braze Alloy

Material Notes: Wide application in soldering.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 11.06 g/cc0.3996 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8.0
@Load 100 kg,
Time 30.0 sec
8.0
@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 27.6 MPa4000 psi
Elongation at Break 45 %45 %
Shear Strength 14.5 MPa2100 psiShear Bond Holding Strength
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000200 ohm-cm0.0000200 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C
@Temperature 20.0 °C
16.7 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 23.0 W/m-K
@Temperature 85.0 °C
160 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 308 - 312 °C586 - 594 °F
Solidus 308 °C586 °F
Liquidus 312 °C594 °F
 
Component Elements PropertiesMetricEnglishComments
Lead, Pb 95 %95 %
Tin, Sn 5.0 %5.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy
Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy
Indium Corp. Indalloy® 165 Pb-Ag-Sn Solder Alloy
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy
Overview of materials for Low Alloy Steel

NNIN47 / 18503

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.