MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion properties are identical and they vary only in work life, cure time and color. They provide excellent adhesion to many primed or painted metal and plastic substrates and are designed to develop sag resistance approximately 30 second after mixing.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 30000 cP30000 cP
Brookfield Viscosity 15000 - 40000 cP15000 - 40000 cPAccelerator, RVF #5 sp @ 20 rpm
 10000 - 55000 cP10000 - 55000 cPBase, RVF #6 sp @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.7 MPa3000 psiASTM D738
Elongation at Break 96 %96 %ASTM D738
Shear Strength  0.138 MPa
@Temperature 82.0 °C
20.0 psi
@Temperature 180 °F
Overlap, Solvent Wiped Steel
 0.276 MPa
@Temperature 82.0 °C
40.0 psi
@Temperature 180 °F
Overlap, Nylon
 0.483 MPa
@Temperature 82.0 °C
70.0 psi
@Temperature 180 °F
Overlap, Plexiglas
 0.689 MPa
@Temperature 82.0 °C
100 psi
@Temperature 180 °F
Overlap, Solvent Wiped Al
 0.689 MPa
@Temperature 82.0 °C
100 psi
@Temperature 180 °F
Overlap, Abraded and Solvent Wiped Steel
 0.758 MPa
@Temperature 82.0 °C
110 psi
@Temperature 180 °F
Overlap, Rigid PVC
 0.758 MPa
@Temperature 82.0 °C
110 psi
@Temperature 180 °F
Overlap, Polystyrene
 0.862 MPa
@Temperature 82.0 °C
125 psi
@Temperature 180 °F
Overlap, Lexan
 1.24 MPa
@Temperature 82.0 °C
180 psi
@Temperature 180 °F
Overlap, FRP
 1.65 MPa
@Temperature -40.0 °C
240 psi
@Temperature -40.0 °F
Overlap, Nylon
 2.07 MPa
@Temperature 82.0 °C
300 psi
@Temperature 180 °F
Overlap
 2.07 MPa
@Temperature 82.0 °C
300 psi
@Temperature 180 °F
Overlap, Etched Aluminum
 2.07 MPa
@Temperature 82.0 °C
300 psi
@Temperature 180 °F
Overlap, Abraded and Solvent Wiped Al
 2.07 MPa
@Temperature 82.0 °C
300 psi
@Temperature 180 °F
Overlap, ABS
 2.28 MPa
@Temperature -40.0 °C
330 psi
@Temperature -40.0 °F
Overlap, Polystyrene
 2.55 MPa
@Temperature -40.0 °C
370 psi
@Temperature -40.0 °F
Overlap, Rigid PVC
 3.03 MPa
@Temperature -40.0 °C
440 psi
@Temperature -40.0 °F
Overlap, ABS, Substrate Failure
 3.65 MPa
@Temperature 24.0 °C
530 psi
@Temperature 75.2 °F
Overlap, Polystyrene
 4.00 MPa
@Temperature 24.0 °C
580 psi
@Temperature 75.2 °F
Overlap, Nylon
 4.27 MPa
@Temperature -40.0 °C
620 psi
@Temperature -40.0 °F
Overlap, Plexiglas
 4.83 MPa
@Temperature 24.0 °C
700 psi
@Temperature 75.2 °F
Overlap, Solvent Wiped Steel
 5.58 MPa
@Temperature 24.0 °C
810 psi
@Temperature 75.2 °F
Overlap, ABS
 6.62 MPa
@Temperature 24.0 °C
960 psi
@Temperature 75.2 °F
Overlap, Rigid PVC
 6.89 MPa
@Temperature -40.0 °C
1000 psi
@Temperature -40.0 °F
Overlap, Solvent Wiped Al
 6.89 MPa
@Temperature -40.0 °C
1000 psi
@Temperature -40.0 °F
Overlap, Solvent Wiped Steel
 6.89 MPa
@Temperature 24.0 °C
1000 psi
@Temperature 75.2 °F
Overlap, Solvent Wiped Al
 7.93 MPa
@Temperature 24.0 °C
1150 psi
@Temperature 75.2 °F
Overlap, FRP, Substrate Failure
 8.27 MPa
@Temperature 24.0 °C
1200 psi
@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Steel
 8.55 MPa
@Temperature -40.0 °C
1240 psi
@Temperature -40.0 °F
Overlap, Lexan, Substrate Failure
 8.96 MPa
@Temperature 24.0 °C
1300 psi
@Temperature 75.2 °F
Overlap, Plexiglas
 11.4 MPa
@Temperature -40.0 °C
1660 psi
@Temperature -40.0 °F
Overlap, FRP, Substrate Failure
 12.7 MPa
@Temperature 24.0 °C
1840 psi
@Temperature 75.2 °F
Overlap, Lexan, Substrate Failure
 13.8 MPa
@Temperature -40.0 °C
2000 psi
@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Steel
 13.8 MPa
@Temperature 24.0 °C
2000 psi
@Temperature 75.2 °F
Overlap
 13.8 MPa
@Temperature 24.0 °C
2000 psi
@Temperature 75.2 °F
Overlap, Etched Aluminum
 13.8 MPa
@Temperature 24.0 °C
2000 psi
@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Al
 13.8 MPa
@Temperature -40.0 °C
2000 psi
@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Al
 17.2 MPa
@Temperature -40.0 °C
2500 psi
@Temperature -40.0 °F
Overlap, Etched Aluminum
 17.2 MPa
@Temperature -55.0 °C
2500 psi
@Temperature -67.0 °F
Overlap
Peel Strength 4.38 kN/m25.0 pliT-Peel
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 min1.50 hour
 1440 min24.0 hourFull Cure
 
Descriptive Properties
AppearanceBrownAccelerator
 Off-WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow ISONATE™ 50 O,P` Pure MDI
Resin Technology Group 404 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Resin Technology Group 24N Two component Polyurethane Adhesive
Resin Technology Group 1121 Two component Polyurethane Adhesive
Dow ISONATE™ 181 MDI Prepolymer

PMM34675 / 169422

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.