MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® XE 4105 black 9992 PA610-GF50
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Product description: Grilamid XE 4105 black 9992 is a 50% glass fiber reinforced, heat stabilized and UV resistant polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materials and its eco-profile is very favorable when compared to similar products based on crude oil. The main features of Grilamid XE 4105 black 9992 are:
  • High stiffness
  • Low water absorption
  • Good heat, UV and chemical resistance
  • Easy processing
Grilamid XE 4105 black 9992 is particularly suitable for the manufacturing of technical injection molded parts in the application fields of:
  • Automotive
  • Electrical & Electronic goods
  • Mechanical engineering
  • Sports & leisure goods
  • Domestic appliances

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³Dry; ISO 1183
Water Absorption 1.9 %1.9 %Sim. to ISO 62
Moisture Absorption 0.800 %0.800 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 175 MPa25400 psiConditioned; ISO 2039-1
 245 MPa35500 psiDry; ISO 2039-1
Tensile Strength at Break 160 MPa23200 psiConditioned; ISO 527-1/-2
 205 MPa29700 psiDry; ISO 527-1/-2
Elongation at Break 3.2 %3.2 %Dry; ISO 527-1/-2
 4.5 %4.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 12.5 GPa1810 ksiConditioned; ISO 527-1/-2
 15.5 GPa2250 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 34.0 kV/mm864 kV/inConditioned; IEC 60243-1
 35.0 kV/mm889 kV/inDry; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1/-2
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 130 °C212 - 266 °FLong Term; ISO 2578
 160 °C320 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 150 °C302 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Automotive electr. and electronics, lighting
 Compressed air systems
 Cooling and climate control
 Exterior
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Lighting
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesBio based Polyamide
Special CharacteristicsImproved heat resistance
 Improved UV resistance (outdoor use)
 Light stabilized or stable to light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Envalior Stanyl® TW240F10 PA46-GF50, Conditioned, 50% Glass Filled, Heat Stabilized
EMS-Grivory Grilamid® XE 4108 black 9992 PA612-GF50
EMS-Grivory Grilamid® XE 3959 nat PA610

PGRH126 / 156835

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.