MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical SEETEC R3410 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Features: Seetec R3410 is a polypropylene-ethylene random copolymer designed for the production of expandable PP and films. It has the good clarity due to the appropriate content of ethylene and offers optimum balance between optical properties and physical strength. Having no slip agent, it is suitable for laminating layer of co-extruded cast film in food packaging or semi retort pouch. SEETEC R3410 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact

Applications: EPP (Expandable PP), Film (Non Slip)

CAS No. 9010-79-1

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D1505
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
Tensile Strength, Yield 26.5 MPa3840 psi50mm/min; ASTM D638
Elongation at Break <= 500 %<= 500 %50mm/min; ASTM D638
Flexural Modulus 0.883 GPa128 ksiASTM D760
Izod Impact, Notched 0.490 J/cm
@Temperature 23.0 °C
0.918 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 144 °C291 °F
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °FASTM D648
Vicat Softening Point 135 °C
@Load 1.00 kg
275 °F
@Load 2.20 lb
ASTM D1525
Flash Point >= 340 °C>= 644 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical SEETEC R3400 Polypropylene Random Copolymer
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer
LG Chemical SEETEC R3450 Polypropylene Random Copolymer
LG Chemical SEETEC H7411 Polypropylene, Homopolymer
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer

PLAY388 / 148398

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.