MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen EP5015 Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen EP5015 is a medium fluidity nucleated heterophasic copolymer suitable for injection molding applications. Moplen EP5015 exhibits an outstanding low temperature impact performance in combination with a good stiffness and an excellent processability. Moplen EP5015 is selected by customers for use in luggage, transport and cold storage crates, sports and leisure equipment, toys and typical consumer goods which require a high impact resistance at low temperatures. Moplen EP5015 resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features Optimized balance of stiffness and toughness/High impact strength at low temperature/High Stiffness/Low warpage/Good whitening resistance

Typical Applications: Crates/Furniture/Luggage/Sports/Leisure and Toys

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 4040ASTM D785
Tensile Strength, Yield 21.1 MPa3060 psiASTM D638
Elongation at Yield 8.0 %8.0 %ASTM D638
Flexural Modulus 1.08 GPa156 ksiASTM D790
Izod Impact, Notched  0.883 J/cm
@Temperature -20.0 °C
1.65 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 125 °C257 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen EP500M Injection Molding Grade Polypropylene
PolyMirae Adstif HA5034 Injection Molding Grade Polypropylene
PolyMirae Clyrell EC340Q Injection Molding Grade Polypropylene
PolyMirae Clyrell EC340R Injection Molding Grade Polypropylene
PolyMirae Moplen EP548P Injection Molding Grade Polypropylene

PMIRAF19 / 183240

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.