MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik DYNACOLL® S 341 HV Copolyester
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Copolyesters: With its DYNACOLL® S product range Evonik offers thermoplastic copolyesters of high molecular weight to a wide variety of thermoplastic hot melt and solvent based applications. The individual grades differ in their melting point, degree of crystallinity and hardness and in their setting time. According to their crystallinity, the product range is arranged into four basic groups:
  • DYNACOLL® S - Highly crystalline grades
  • DYNACOLL® S - Moderately crystalline grades
  • DYNACOLL® S - Slightly crystalline grades
  • DYNACOLL® S - Amorphous grades
DYNACOLL® S copolyesters are generally supplied as granules, usually in bags of 20 or 25 kg. They can be processed into following forms of applications: adhesive film, web or net, powder, paste, hot melt and solution.

Your benefits: DYNACOLL® S - Moderately crystalline grades

  • moderate open times
  • very good adhesive strength and heat resistance

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  10 cP
@Temperature 220 °C
10 cP
@Temperature 428 °F
DIN EN ISO 3219
 20 cP
@Temperature 200 °C
20 cP
@Temperature 392 °F
DIN EN ISO 3219
 30 cP
@Temperature 180 °C
30 cP
@Temperature 356 °F
DIN EN ISO 3219
Viscosity Number 80 cm³/g0.80 dl/gDIN 53728
Melt Flow  200 g/10 min
@Load 2.20 kg,
Temperature 180 °C
200 g/10 min
@Load 4.85 lb,
Temperature 356 °F
DIN ISO 1133
 300 g/10 min
@Load 2.20 kg,
Temperature 200 °C
300 g/10 min
@Load 4.85 lb,
Temperature 392 °F
DIN ISO 1133
 500 g/10 min
@Load 2.20 kg,
Temperature 220 °C
500 g/10 min
@Load 4.85 lb,
Temperature 428 °F
DIN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555DIN 53505
Tensile Strength at Break 15.0 MPa2180 psiDIN EN ISO 527-1/3
Elongation at Break 50 %50 %DIN EN ISO 527-1/3
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °FDIN 53765
Softening Point 160 °C320 °FDIN ISO 4625
Glass Transition Temp, Tg -30.0 °C-22.0 °FDIN 53765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik DYNACOLL® S 341 Copolyester
Evonik DYNACOLL® 7111 Copolyester
Envalior Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America)
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)

PEVONIL088 / 196292

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.