MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reliance Industries Relene E41003 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial effluent as per IS 4984:1995, IS 14151:1995 and IS 14333:1996.

Information provided by Reliance Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.943 g/cc0.0341 lb/in³ASTM D1505
Melt Flow 0.28 g/10 min
@Load 2.16 kg
0.28 g/10 min
@Load 4.76 lb
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 64.564.5ASTM D2240
Tensile Strength, Ultimate 24.0 MPa3480 psiASTM D638
Tensile Strength, Yield 20.0 MPa2900 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Flexural Modulus 0.700 GPa102 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 124 °C255 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reliance Industries Reclair F18010 Polyethylene
Reliance Industries Relene B31101 Polyethylene
Reliance Industries Relene M60075 Polyethylene
Reliance Industries Relene S42005 Polyethylene
Reliance Industries Relene B56003 Polyethylene

PREL068 / 65408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.