MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion BrushBronze® 630 (AMS 4640) 0.250" - 1.0"  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: Information supplied by Brush Wellman Engineered Materials.

BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading conditions. This material, specified as AMS 4640, is frequently used for very demanding aerospace applications, including, but not limited to: bushings, spherical and rod end bearings, rub pads, and wear strips. This material is also commonly used for applications in the oil and gas and other durable goods markets.

BrushBronze™ 630 (AMS 4640) offers several significant advantages over other materials available in the marketplace due to the EquaCast™ process:

  • Higher and more consistent mechanical properties
  • Improved service life
  • Ease of use

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 201 - 248201 - 248
Tensile Strength, Ultimate 758 MPa110000 psi
Tensile Strength, Yield 469 MPa68000 psi
Elongation at Break 10 %10 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 9.0 - 11 %9.0 - 11 %
Copper, Cu >= 78 %>= 78 %
Iron, Fe 2.0 - 4.0 %2.0 - 4.0 %
Manganese, Mn <= 1.5 %<= 1.5 %
Nickel, Ni 4.0 - 5.5 %4.0 - 5.5 %
Silicon, Si <= 0.25 %<= 0.25 %
Tin, Sn <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.30 %<= 0.30 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion BrushBronze® 630 (AMS 4640) 1.0" - 2.0"
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 25.4 - 50.8 mm.
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 50.8 - 76.2 mm.
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, ≤ 25.4 mm.

NBB250 / 15113

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.