MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omnia Plastica PTFE Polytetrafluoroethylene
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.

Features:

  • Chemical: a typical fluoropolymer with very high chemical resistance. Mechanical: the mechanical features such as tensile stress and compressive strength are poor. Notably the bearing strain is very low.
  • Very good resistance to low and high temperatures up to 260° C. as well as to UV rays.
  • Low flammability
  • Low friction coefficient
  • Colour: natural
Weak Point:

Poor mechanical properties. The strain is very high, even simply under the weight of the piece.

Application:

  • Chemical: very high chemical resistance to alkali and acids is the main feature of the fluoropolymers. PTFE is used for parts in the petrochemical and chemical industries.
  • Food contact: physiologically inert it is approved for use in contact with food by some standards, whilst in some countries this use is questioned.
  • Electrical: very good dielectric, self-extinguishing and weather stability properties make it suitable for this field.
  • Mechanical: the low friction coefficient makes it suitable for bearings, provided that they work under low charge.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.18 g/cc0.0788 lb/in³ISO.1183 DIN.53479
Moisture Absorption at Equilibrium 0.00 %0.00 %50% relative humidity
Water Absorption at Saturation 0.00 %0.00 %23°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353dry sample; ISO2039.2
Ball Indentation Hardness 30.0 MPa4350 psiISO2039.1 DIN.53456
Tensile Strength at Break 20.0 MPa2900 psiISO.527 DIN.53455
Elongation at Break 500 %500 %ISO.527 DIN.53455
Tensile Modulus 0.700 GPa102 ksiISO.527 DIN.53455
Compressive Strength 1.50 MPa218 psi1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NBNB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.100.10on dry ground steel; load =0.05MPa; speed =0.6 m/s
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmISO.93 DIN.53482
Dielectric Constant 2.1
@Frequency 1e+6 Hz
2.1
@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 11.0 kV/mm279 kV/inISO.243 DIN.53481
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
7.78 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FDIN.52612
Melting Point 325 °C617 °F
Maximum Service Temperature, Air 250 °C482 °FContinuous; 5000 hours based on a tensile stress of 50% at 23° C.
 260 °C500 °Fshort period, no load
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO.75 DIN.53461
Minimum Service Temperature, Air -200 °C-328 °Fimpact conditions and heavy loads not considered
Flammability, UL94 V-0V-0
Oxygen Index 92 %92 %ISO.4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Rulon® J Bearing/Seal PTFE
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Molded

POMNIA32 / 55622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.