MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Terblend® N NM-19XP is an ABS/PA blend with excellent impact toughness, very good flowability and UV-stabilization. High impact strength, Easy processing, UV-stabilized.

Applications: Unpainted automotive interior parts, Center consoles, Air inlets, Steering wheel covers

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.2 %
@Temperature 23.0 °C
1.2 %
@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inISO 294-4
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/inISO 2577
Melt Flow 40 g/10 min
@Load 10.0 kg,
Temperature 240 °C
40 g/10 min
@Load 22.0 lb,
Temperature 464 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ISO 2039-2
Ball Indentation Hardness 86.0 MPa12500 psiISO 2039-1
Tensile Strength, Yield 43.0 MPa6240 psiISO 527
Elongation at Break 30 %30 %ISO 527
Elongation at Yield 3.5 %3.5 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Flexural Strength 62.0 MPa8990 psiISO 178
Flexural Modulus 1.80 GPa261 ksiISO 178
Izod Impact, Notched (ISO)  15.0 kJ/m²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 65.0 kJ/m²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C55.6 µin/in-°FISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  102 °C
@Load 5.10 kg
216 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 160 °C
@Load 1.02 kg
320 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °FISO 294
Mold Temperature 40.0 - 80.0 °C104 - 176 °FISO 294
 
Descriptive Properties
ColorBeige 38163
Commercial StatusEurope
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terblend® N NM-19 ABS/PA6 (Dry)
INEOS Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Conditioned)
INEOS Styrolution Terblend® N NM-19 ABS/PA6 (Conditioned)
INEOS Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Dry)
INEOS Styrolution Terblend® N NM-11 ABS/PA6 (Dry)

PBASG0605 / 132238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.