MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with PTFE Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.42 - 2.03 g/cc0.0513 - 0.0733 lb/in³Average value: 1.58 g/cc Grade Count:21
Filler Content 10.0 - 70.0 %10.0 - 70.0 %Average value: 35.8 % Grade Count:14
Linear Mold Shrinkage 0.00200 - 0.0200 cm/cm0.00200 - 0.0200 in/inAverage value: 0.0114 cm/cm Grade Count:15
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 64.0 - 84.064.0 - 84.0Average value: 71.5 Grade Count:4
Tensile Strength, Ultimate 11.0 - 160 MPa1600 - 23200 psiAverage value: 49.8 MPa Grade Count:23
Elongation at Break 0.500 - 68.0 %0.500 - 68.0 %Average value: 5.04 % Grade Count:23
Modulus of Elasticity 1.65 - 15.0 GPa240 - 2180 ksiAverage value: 4.76 GPa Grade Count:20
Flexural Yield Strength 18.6 - 180 MPa2700 - 26100 psiAverage value: 75.9 MPa Grade Count:21
Flexural Modulus 1.31 - 15.0 GPa190 - 2180 ksiAverage value: 4.07 GPa Grade Count:19
Flexural Strain at Break 1.30 - 8.00 %1.30 - 8.00 %Average value: 4.15 % Grade Count:4
Izod Impact, Notched 0.160 - 0.641 J/cm0.300 - 1.20 ft-lb/inAverage value: 0.309 J/cm Grade Count:13
Izod Impact, Unnotched 1.07 - 3.74 J/cm2.00 - 7.00 ft-lb/inAverage value: 2.14 J/cm Grade Count:11
Charpy Impact Unnotched 1.00 - 4.00 J/cm²4.76 - 19.0 ft-lb/in²Average value: 2.17 J/cm² Grade Count:3
Charpy Impact, Notched 0.150 - 1.00 J/cm²0.714 - 4.76 ft-lb/in²Average value: 0.517 J/cm² Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cm1.00e+12 - 1.00e+16 ohm-cmAverage value: 1.76e+15 ohm-cm Grade Count:7
Surface Resistance 1.00e+12 - 1.00e+15 ohm1.00e+12 - 1.00e+15 ohmAverage value: 3.00e+14 ohm Grade Count:4
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 - 270 °C199 - 518 °FAverage value: 147 °C Grade Count:16
Flammability, UL94 HB - V-0HB - V-0Grade Count:14
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 343 °C536 - 650 °FAverage value: 318 °C Grade Count:16
Mold Temperature 130 - 180 °C266 - 356 °FAverage value: 152 °C Grade Count:17
Drying Temperature 50.0 - 160 °C122 - 320 °FAverage value: 136 °C Grade Count:16
Moisture Content 0.0200 - 0.0400 %0.0200 - 0.0400 %Average value: 0.0375 % Grade Count:8
Injection Pressure 30.0 - 103 MPa4350 - 15000 psiAverage value: 83.6 MPa Grade Count:12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Mitsubishi Chemical Advanced Materials Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet)
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled

O4554 / 78356

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.