MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niagara LaSalle 1215 Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel

Material Notes: The A.I.S.I. grade 1215 has essentially eliminated a number of similar free machining grades, such as 1212. Both 1215 and 1213 machine considerably faster than 1212 and provide good surface finish and brazing properties. These steels are difficult to weld and are not recommended for case hardening. They are generally used where mechanical properties can be sacrificed for machinability.

Information provided by Niagra LaSalle Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 167167
Tensile Strength 538 MPa78000 psi
Tensile Strength, Yield 414 MPa60000 psi
Elongation at Break >= 10 %>= 10 %2"
Reduction of Area 35 %35 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.090 %<= 0.090 %
Iron, Fe 98.42 - 98.95 %98.42 - 98.95 %as balance
Manganese, Mn 0.75 - 1.05 %0.75 - 1.05 %
Phosphorus, P 0.040 - 0.090 %0.040 - 0.090 %
Sulfur, S 0.26 - 0.35 %0.26 - 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1215 Steel, cold drawn, 19-38 mm round
AISI 12L14 Steel, cold drawn, 19-38 mm round
AISI 1215 Steel, drawn, ground, and polished, 19-38 mm round
AISI 1215 Steel, turned and polished, 19-38 mm round
AISI 1213 Steel, cold drawn, 19-38 mm round

NNIAL012 / 160302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.