MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Denka MALECCA K-200 ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had defects in terms of moldability, thermal stability, and impact resistance.

Applications

  • Mobile phones
  • vehicle-mounted audio equipment
  • automotive interior components
  • home electric appliances
  • OA equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
 114114ISO 2039-2
Tensile Strength at Break 41.0 MPa5950 psiASTM D638
 48.0 MPa6960 psi50mm/min; ISO 527-2
Tensile Strength, Yield 39.0 MPa5660 psiISO 527-2
Elongation at Break 28 %28 %ISO 527-2
Tensile Modulus 2.50 GPa363 ksi1mm/min; ISO 527-1
Flexural Strength 75.0 MPa10900 psi15mm/min; ASTM D790
 78.0 MPa11300 psiISO 178
Flexural Modulus 2.35 GPa341 ksi15mm/min; ASTM D790
 2.45 GPa355 ksi2mm/min; ISO 178
Izod Impact, Notched 1.96 J/cm
@Temperature 23.0 °C
3.67 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched 1.90 J/cm²9.04 ft-lb/in²ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-2
 106 °C223 °FASTM D648
Vicat Softening Point 115 °C239 °F50N; ISO 306
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka MALECCA K-100 ABS
Denka MALECCA K-096 ABS
Denka MALECCA K-090 ABS
Overview of materials for Nylon 66, Extruded
Overview of materials for AISI 4000 Series Steel

PDENK004 / 29668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.