MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® BU50I PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU50I makes it ideal for applications in which the weld line impact strength at low temperatures is critical.

Applications: Automotive components, small engines, power tool parts and casings, cold weather and high impact supports gear, such as snowboards, ski components, helmets and hockey masks.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Moisture Absorption at Equilibrium 2.1 %2.1 %50% RH; ASTM D570
 7.3 %7.3 %Saturation; ASTM D570
Linear Mold Shrinkage 0.04572 cm/cm0.04572 in/in1/8" bar
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break >= 100 %>= 100 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Strength 65.0 MPa9430 psiASTM D790
Flexural Modulus 1.69 GPa245 ksiASTM D790
Izod Impact, Notched (ISO)  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy 264 J195 ft-lbBASF
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FASTM D648
UL RTI, Electrical 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 1.50 mm
149 °F
@Thickness 0.0591 in
746B
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 300 °C518 - 572 °F
Mold Temperature 60.0 - 85.0 °C140 - 185 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.15 %<= 0.15 %
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® BU50I PA6 (Conditioned)
Teknor Apex Chemlon® 253 Nylon 6, Toughened
BASF Ultramid® BU50I BK 106 PA6 (Conditioned)
Teknor Apex Chemlon 275 Nylon 6, Copolymer Impact Modified
BASF Ultramid® BU50I BK 106 PA6 (Dry)

PBASG0439 / 132072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.