Hostacom EYS 2004L 105518 is an unfilled copolymer with high melt flow rate, high gloss, and high scratch resistance. The grade is being in development status, this is a preliminary datasheet subjected to changes after product industrialization. Applications: AppliancesInformation provided by LyondellBasell. |