MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 3105-H16
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A93105; ISO AlMn0.5Mg0.5; Aluminium 3105-H16; AA3105-H16; Al3105-H16
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.72 g/cc0.0983 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 5353500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 6868Converted from Brinell Hardness Value
Tensile Strength, Ultimate 193 MPa28000 psiAA; Typical
Tensile Strength, Yield 172 MPa25000 psiAA; Typical
Elongation at Break 4.0 %
@Thickness 1.59 mm
4.0 %
@Thickness 0.0625 in
AA; Typical
Modulus of Elasticity 68.9 GPa10000 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.330.33
Shear Modulus 25.0 GPa3630 ksi
Shear Strength 110 MPa16000 psiAA; Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000382 ohm-cm
@Temperature 20.0 °C
0.00000382 ohm-cm
@Temperature 68.0 °F
AA; Typical
Magnetic Susceptibility 7.0e-77.0e-7cgs/g at 20ºC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.1 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.5 µm/m-°C
@Temperature 20.0 - 200 °C
13.6 µin/in-°F
@Temperature 68.0 - 392 °F
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.897 J/g-°C0.214 BTU/lb-°F
Thermal Conductivity 171 W/m-K1190 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 635.0 - 654 °C1175 - 1210 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 635.0 °C1175 °FAA; Typical
Liquidus 654 °C1210 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 °C650 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 95.9 %<= 95.9 %As remainder
Chromium, Cr <= 0.20 %<= 0.20 %
Copper, Cu <= 0.30 %<= 0.30 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg 0.20 - 0.80 %0.20 - 0.80 %
Manganese, Mn 0.30 - 0.80 %0.30 - 0.80 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.60 %<= 0.60 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.40 %<= 0.40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 3105-H24
Aluminum 3105-H26
Aluminum 3105-O
Aluminum 3105-H28
Aluminum 3105-H12

MA3105H16 / 9040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.