MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Udel® P-1750 MR Polysulfone (PSU)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.

Polysulfones have long been known for transparency and clarity, but have been somewhat limited by a slight yellow cast which has been typical of the material. These grades were designed to eliminate the yellow cast and provide improved aesthetics for applications where a yellow cast is undesirable.

Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Good Chemical Resistance; Good Toughness; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable

Uses: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Parts; Microwave Cookware; Piping; Plumbing Parts; Valves/Valve Parts

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/in
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 343 °C
6.5 g/10 min
@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.3 MPa10200 psiASTM D638
Elongation at Break 50 - 100 %50 - 100 %ASTM D638
Tensile Modulus 2.48 GPa360 ksiASTM D638
Flexural Strength 106 MPa15400 psiASTM D790
Flexural Modulus 2.69 GPa390 ksiASTM D790
Izod Impact, Notched 0.690 J/cm1.29 ft-lb/inASTM D256
Tensile Impact Strength 420 kJ/m²200 ft-lb/in²ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+16 ohm-cm3.00e+16 ohm-cmASTM D257
Dielectric Constant  2.9
@Frequency 60 Hz
2.9
@Frequency 60 Hz
ASTM D150
 3.02
@Frequency 1e+6 Hz
3.02
@Frequency 1e+6 Hz
ASTM D150
 3.04
@Frequency 1000 Hz
3.04
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
ASTM D150
 0.0070
@Frequency 60 Hz
0.0070
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C31.1 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 174 °C345 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 329 - 385 °C624 - 725 °F
Mold Temperature 121 - 163 °C250 - 325 °F
Drying Temperature 135 - 163 °C
@Time 12600 sec
275 - 325 °F
@Time 3.50 hour
Shot Size 50 - 75 %50 - 75 %
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorClear/Transparent
FormPellets
Processing TechniqueExtrusion; Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® S 3010 PSU
Syensqo (Solvay Specialty Polymers) Udel® P-1835 Polysulfone (PSU)
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Syensqo (Solvay Specialty Polymers) Udel® P-1720 Polysulfone (PSU)
Syensqo (Solvay Specialty Polymers) Udel® P-1800 Polysulfone (PSU)

PSOL8Y7376 / 177107

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.