MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 7142 Repositionable Paper Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Repositionable Paper Label Material 7113 and 7142 with 3M™ Adhesive 1000 offer unique, one-piece removability from many surfaces, including fragile papers, and can be repositioned repeatedly for reuse on the same surface or application to another surface.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 63.5 microns2.50 milLiner
 102 microns4.00 milFacestock
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.0110 kN/m0.0625 pliCorrugated Board, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.0110 kN/m0.0625 pliKraft Paper, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.0110 kN/m0.0625 pliCorrugated Board, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.0110 kN/m0.0625 pliKraft Paper, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.0219 kN/m0.125 pliCellophane, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.0219 kN/m0.125 pliGlass, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.0219 kN/m0.125 pliBond Paper, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.0219 kN/m0.125 pliBond Paper, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.027391 kN/m0.15625 pliPolypropylene, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.027391 kN/m0.15625 pliCellophane, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.03287 kN/m0.1875 pliAcrylic, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.03287 kN/m0.1875 pliPainted Metal, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 0.03287 kN/m0.1875 pliPolypropylene, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.03287 kN/m0.1875 pliGlass, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.03287 kN/m0.1875 pliPainted Metal, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.03287 kN/m0.1875 pliStainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.05478 kN/m0.3125 pliAcrylic, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 0.0877 kN/m0.500 pliStainless Steel, 180° Peel, Conditioned for 3 days at 49³C; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= -15.0 °C>= 5.00 °FApplication
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type1000 repositionable acrylic
Liner40# kraft glassine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Miracll H206 Thermoplastic Polyurethane Hot Melt/Solvent Adhesive
Michelman® Michem® Coat 40Y Water resistant, cold set and hot melt gluable coating
Kolon CY201 Silicone Release Film
Chemical Concepts Chem-Set™ 707 High Performance Hot Melt
Chemical Concepts Chem-Set™ 601 Low Temperature Hot Melt Adhesive

PMM33626 / 168373

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.