MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celstran® PA6-GF30-01 Nylon 6, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: 30% long strand glass fiber reinforced nylon 6 Black

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cm0.00050 - 0.0010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 155 MPa22500 psi5mm/min; ISO 527-2/1A
 203 MPa29500 psiASTM D638
 87.6 MPa
@Temperature 121 °C
12700 psi
@Temperature 250 °F
ASTM D638
 230.8 MPa
@Temperature -40.0 °C
33470 psi
@Temperature -40.0 °F
ASTM D638
Elongation at Break 1.78 %1.78 %5mm/min; ISO 527-2/1A
 2.6 %2.6 %ASTM D638
 3.0 %
@Temperature 121 °C
3.0 %
@Temperature 250 °F
ASTM D638
 3.1 %
@Temperature 4.44 °C
3.1 %
@Temperature 40.0 °F
ASTM D638
Tensile Modulus 9.51 GPa1380 ksi50mm/min; ISO 527-2/1A
 10.3 GPa1500 ksiASTM D638
 5.79 GPa
@Temperature 121 °C
840 ksi
@Temperature 250 °F
ASTM D638
 9.65 GPa
@Temperature -40.0 °C
1400 ksi
@Temperature -40.0 °F
ASTM D638
Flexural Strength 290 MPa42100 psiASTM D790
 130 MPa
@Temperature 121 °C
18800 psi
@Temperature 250 °F
ASTM D790
 318.7 MPa
@Temperature -40.0 °C
46230 psi
@Temperature -40.0 °F
ASTM D790
Flexural Modulus 8.83 GPa1280 ksiISO 178
 9.03 GPa1310 ksiASTM D790
 4.00 GPa
@Temperature 121 °C
580 ksi
@Temperature 250 °F
ASTM D790
 9.79 GPa
@Temperature -40.0 °C
1420 ksi
@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 2.62 J/cm4.90 ft-lb/inASTM D256
 2.35 J/cm
@Temperature -40.0 °C
4.40 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 3.84 J/cm
@Temperature 121 °C
7.20 ft-lb/in
@Temperature 250 °F
ASTM D256
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 207 °C405 °FISO 75-1, -2
 207 °C405 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 100 °C176 - 212 °Fcavity
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 260 - 270 °C500 - 518 °F
Zone 2 265 - 275 °C509 - 527 °F
Zone 3 270 - 280 °C518 - 536 °F
Zone 4 270 - 280 °C518 - 536 °F
Die Temperature 270 - 280 °C518 - 536 °F
Melt Temperature 270 - 280 °C518 - 536 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.18 %<= 0.18 %
 
Descriptive Properties
Injection moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 73G30HSL BK261 PA6-GF30
Envalior Novamid® 1013GMF H2 NAT/BK37 PA6-GF30
Avient Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE)
Envalior Akulon® K224-G6 PA6-GF30, Dry, 30% Glass Filled
Celanese Zytel® 73G30HSL NC010 PA6-GF30

PHCQ181 / 178636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.