MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: PA 6T/66 Acc. to ASTM: PPA, polyphthalamide The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. Grivory HT is suitable for production of technical parts in the application fields of:
  • Electro
  • Electronics
  • Automotive
  • Safety technology
  • Mechanical engineering

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³Dry; ISO 1183
Water Absorption 5.0 %5.0 %Sim. to ISO 62
Moisture Absorption 1.80 %1.80 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 250 MPa36300 psiConditioned; ISO 2039-1
 270 MPa39200 psiDry; ISO 2039-1
Tensile Strength at Break 165 MPa23900 psiConditioned; ISO 527-1/-2
 175 MPa25400 psiDry; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %Dry; ISO 527-1/-2
 2.0 %2.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 11.0 GPa1600 ksiDry; ISO 527-1/-2
 11.0 GPa1600 ksiConditioned; ISO 527-1/-2
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 38.0 kV/mm965 kV/inDry; IEC 60243-1
 38.0 kV/mm965 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C38.9 µin/in-°FISO 11359-1/-2
Melting Point 310 °C590 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °C284 °FLong Term; ISO 2578
 270 °C518 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 200 °C392 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveExterior
 Fuel systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Special CharacteristicsImproved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50
EMS-Grivory Grivory® HT2V-3H LF PA*-GF30
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30
Evonik VESTAMID® HTplus M3033 PA10T/X, GF30
Celanese Zytel® HTN52G35HSL BK083 PA6T/66-GF35

PGRH383 / 157092

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.