MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems DuraForm® ProX® PA Plastic
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Strong, tough plastic that stands up to the rigors of long-term real world use replacing traditionally injection molded articles.

Applications: Functional prototyping and low volume production parts for automotive, aerospace and consumer goods, as well as housings, enclosures, connectors, snapfits and complex assemblies.

Features:

  • Excellent mechanical properties
  • Outstanding surface smoothness
  • Stable dimensional and mechanical properties over time
  • Exceptional recyclability
  • Very high part density
  • ISO 10993-5 and ISO 10993-10 capable
  • Suitable for manufacture of select medical devices
Benefits:
  • Replace articles that are typically CNC machined or injection molded with this tough plastic
  • Exceptional recycling rate reduces waste and decreases production costs
  • Expanded utilization of parts

Information provided by 3D Systems

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³Sintered Part
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373ASTM D 2240
Tensile Strength at Break 50.0 MPa7250 psiASTM D 638
Tensile Strength, Ultimate 50.0 MPa7250 psiASTM D 638
Elongation at Break 22 %22 %ASTM D 638
Elongation at Yield 14 %14 %ASTM D 638
Tensile Modulus 1.77 GPa257 ksiASTM D 638
Flexural Strength 60.0 MPa8700 psiASTM D 790
Flexural Modulus 1.65 GPa239 ksiASTM D 790
Izod Impact, Notched 0.450 J/cm0.843 ft-lb/in0.12; ASTM D256
Izod Impact, Unnotched 6.44 J/cm
@Thickness 3.05 mm
12.1 ft-lb/in
@Thickness 0.120 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.46e+15 ohm-cm1.46e+15 ohm-cmASTM D257
Surface Resistance 4.66e+15 ohm4.66e+15 ohmASTM D257
Dielectric Constant 2.85
@Frequency 1000 Hz
2.85
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 15.2 kV/mm386 kV/inASTM D149
Dissipation Factor 0.022
@Frequency 1000 Hz
0.022
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  109.5 µm/m-°C
@Temperature 0.000 - 50.0 °C
60.83 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831
 221.7 µm/m-°C
@Temperature 85.0 - 145 °C
123.2 µin/in-°F
@Temperature 185 - 293 °F
ASTM E831
Specific Heat Capacity 1.55 J/g-°C0.370 BTU/lb-°FASTM E1269
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°FASTM E1530
Deflection Temperature at 0.46 MPa (66 psi) 182 °C360 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FASTM D 648
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems DuraForm® ProX® HST Composite Thermoplastic Elastomer for SLS® Systems
3D Systems DuraForm® ProX® GF Plastic Glass Filled Plastic for SLS® Systems
3D Systems DuraForm® ProX® FR1200 Flame-retardant nylon 12
3D Systems DuraForm® ProX® AF+ Aluminum filled nylon 12 plastic
3D Systems DuraForm® ProX EX BLK Nylon 11 based plastic

PAPPR3154 / 239122

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.