MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular material which, while it can be used for film production, is also suitable for compounding.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 3500 ppm
  • Slip: 1500 ppm
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Bag in Box
  • Blown Film
  • Cast Film
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • Garment Film
  • General Packaging
  • Industrial Packaging
  • Liners
  • Mulch Film
  • Packaging Films
  • Produce Bags on a Roll
  • Shoppers
  • Trash Can Liners

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ExxonMobil method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 3500 ppm3500 ppm
Slip Level 1500 ppm1500 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.27 MPa1200 psiASTM D882
Film Tensile Strength at Yield, TD 8.27 MPa1200 psiASTM D882
Film Elongation at Break, MD 660 %660 %ASTM D882
Film Elongation at Break, TD 780 %780 %ASTM D882
Puncture Energy 1.10 J0.808 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 120 g120 gASTM D1922
Elmendorf Tear Strength TD 340 g340 gASTM D1922
Dart Drop Test 70.0 g0.154 lbASTM D1709A
Film Tensile Strength at Break, MD 36.5 MPa5300 psiASTM D882
Film Tensile Strength at Break, TD 26.2 MPa3800 psiASTM D882
1% Secant Modulus, MD 179 MPa26000 psiASTM D882
1% Secant Modulus, TD 193 MPa28000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 123 °C<= 253 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 29 %29 %ASTM D1003
Gloss 22 %22 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film
ExxonMobil NTX™ NTX 095 Super Strength Film Resin
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin

PEX99147 / 175383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.